How to make the abrasive tools that have been made soft down?
USD $1 - $2 /Piece
Min.Order:1 Piece
The ceramic bond abrasive is immersed in a sodium hydroxide or potassium hydroxide solution, heated to the boiling point, and the concentration of the alkali solution and the boiling time are controlled to appropriately reduce the hardness of the abrasive. Refer to Table 1 for the compatible concentration boiling time.
If you need any products, do not hesitate to contact
Annamoresuper@gmail.com
@moresuperhard.com
WhatsApp:+8615617785923
Skype:Annawng
Wechat:15617785923
QQ:1664333593
Mobile:+86-156177854923
Tel/Fax:+86-0371-86545906
Table 1 Alkali treatment to reduce the hardness of the abrasive reference table | |||||||||||
Abrasive Grit | Boiling time(h) | Original hardness of abrasive tool | |||||||||
K | L | M | N | P | Q | R | S | T | Y | ||
Alkaline concentration(%) | |||||||||||
10 | 20 | 30 | 10 | 20 | 30 | 10 | 20 | 30 | 40 | ||
24# | 124 | 123 | 234 | 234 | 113 | 123 | 223 | 123 | 234 | 345 | 235 |
46# | 124 | 234 | 345 | 356 | 134 | 234 | 245 | 112 | 123 | 234 | 123 |
60# | 124 | 123 | 234 | 346 | 123 | 234 | 235 | 112 | 123 | 233 | 133 |
The strength of the grinding wheel after the treatment will be reduced. Therefore, it must be passed after passing the rotary inspection, especially the grinding wheel with a hardness reduction of 3~4, and more attention should be paid to prevent the grinding wheel from breaking when it is used.