ASTM A213 T21 Seamless alloy tube
USD $1000 - $3000 /Ton
Min.Order:10 Tons
Sunny Steel PipeFitting Industires
ASTM A213 T21 is the part of ASTM A213 Standard Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, Heat-Exchanger Tubes.
ASTM A213 T21 Grades containing the letter H in their designation have requirements different from those of similar grades not containing the letter H.
These different requirements provide higher creep-rupture strength than normally achievable in similar grades without these different requirements. ASTM A213 T21tubes shall be made by the seamless process and shall be either hot finished or cold finished, as specified. Grade TP347HFG shall be cold finished. Heat treatment shall be done separately and in addition to heating for hot forming. The ferritic alloy and ferritic stainless steels shall be reheated. On the other hand, austenitic stainless steel tubes shall be furnished in the heat-treated condition. Alternatively, immediately after hot forming, while the temperature of the tubes is not less than the minimum solution temperature, tubes may be individually quenched in water or rapidly cooled by other means. Tension test, hardness test, flattening test, and flaring test shall be done to each tube. Also, each tube shall be subjected to the nondestructive electric test or hydrostatic test.
Other standard specifications include the categories of A209 seamless carbon-molybdenum alloy-steel boiler and superheater tubes; A210 seamless medium-carbon steel boiler and superheater tubes and A213 seamless ferritic and austenitic steel boiler, superheater and heat-exchanger tubes.
Piping wall thicknesses range from 1/2 inch to 5 inches. A213 grades also have the letter H or M assigned, which changes the composition and specifications for that series.
This abstract is a brief summary of the referenced standard. It is informational only and not an official part of the standard; the full text of the standard itself must be referred to for its use and application.
For pipe whose diameter exceeds NPS 25 and whose diameter to wall thickness ratio is 7.0 or less shall be subjected to the bend test instead of the flattening test.
Other pipe whose diameter equals or exceeds NPS 10 may be given the bend test in place of the flattening test subject to the approval of the purchaser.
The bend test specimens shall be bent at room temperature through 180 without cracking on the outside of the bent portion.
Packed in wooden crates, wrapped in plastic, and suitably protected for sea-worthly delivery or as requested.
Both ends of each crate will indicate the order no., heat no., dimensions, weight and bundles or as requested.
ASTM A213, ASTM A213 T91, ASTM A213 T22, ASTM A213 T12, ASTM A213 T11, ASTM A213 T9, ASTM A213 T5