Solution & Melt Dry-jet Wet Spinning Tester
Negotiable
Min.Order:1
Model | AT236 |
Viscosity of spinning solution | 50-200Pa.s |
Monofilament fineness | 0.1-1mm |
Spinning speed | 5m/min-100m/min |
Spinning Temperature | <450 ℃ |
Far Infrared Ceramic Heating Box Temperature | <550 ℃ |
Power supply | 200V, 50Hz |
Pakeging | ||
1. The equipment is covered with film is protect it from water vapour during the trip. 2. The box is filled with foam to protect the equipment from impact. 3. Exported wooden box made from plywood, don't need fumigated. |