2 mm~5 mm Sino Erli SS E309L Titanium calcium type coating welding electrode E309L-16/ISO 3581-B-ES 309L-16
Negotiable
Min.Order:1
Sino Erli Industrial And Trading Co., Ltd.
2 mm~5 mm Sino Erli Stainless steel E304 Titanium calcium type coating welding electrode
2 mm~5 mm Sino Erli Stainless steel A607 alkaline coating welding electrode GB/T 983 E330MoMnWNb-15
0.8 mm~3.2 mm Sino Erli TG308 tig pure Argon Arc stainless steel 308 welding wire S308/ ER308
0.8 mm~3.2 mm Sino Erli MG410 Mag Argon Oxygen stainless steel 410 welding wire S410/ ER410
0.8 mm~3.2 mm Sino Erli MG430 Mag Argon Oxygen MIG stainless steel 410 welding wire S410/ ER410
E309L is an ultra-low carbon Cr23Ni13 stainless steel electrode with titanium calcium coating. It has excellent crack resistance. AC and DC dual purpose, capable of all-position welding
Commonly used for welding of stainless steel and other dissimilar steels, and also for welding of transition layers of petrochemical pressure vessels and other equipment
Item | C | Mn | Si | Cr | Ni | Mo | P | S | Cu |
Guarantee value | ≤ 0.04 |
0.50~2.50 | ≤1.00 | 22.0~25.0 | 12.0~14.0 | ≤0.75 | ≤0.040 | ≤0.030 | ≤0.75 |
Typical value | 0.023 | 1.75 | 0.70 | 23.75 | 13.40 | 0.047 | 0.021 | 0.009 | 0.036 |
Rm (MPa) | A(%) |
≥510 | ≥25 |
590 | 40 |
Attention:
1. The electrode must be baked at 300°C for 1 hour before welding, and used as it is baked.
2. Try to use small current and short arc welding when welding.
3. The weldments must be cleaned of rust, oil stains, moisture and other impurities before welding.
4. Try to use small current and short arc when welding, and the swing width should not exceed 2.5 times the diameter.