Nickel Chrome Alloy Ni80Cr20
Negotiable /Kilogram
Min.Order:50 Kilograms
Changzhou Brilliance Special Steel Co., Ltd.
Production Description:
Such electrothermal alloy has stable structure and electrical physical property. It has so good high temperature mechanical property, fine cold plastic deformation and weldableness that brittle fracture won't occur even used for long. The alloy is widely used in manufacturing the household appliances and heating element whose working temperature is below 1000ºC. Moreover, it has long lifespan.
Density:8.40g/cm³
Also, with advanced equipment and technology, we can serve you other products as follows:
1. Super alloys (Casting master alloy, deformation super alloy and so on).
2. Corrosion resistant alloy.
3. Welding wire.
4. Precision alloys (soft magnetic alloy, expansion alloy and so on).
5. High resistance alloys for electrical heating.
Our advantage:
1. Experienced manufacturer
2. Stable products and service quality
3. Timely delivery
4. Good technology support
5. Win-win cooperation opportunity
Size:
Hot-rolled bar: Φ 8~38mm
Cold-drawn bar: ≤ 50mm
Forging bar: Φ 38~350mm
Wire: Φ 0.1mm~18mm
Cold-rolled strip: 0.15~4× 200mm
Hot-rolled strip: 4~22× 200mm
Cold-rolled sheet: 0.5~4× 1000× 2000mm
Hot-rolled sheet: 4~22× 1000× 2000mm
Feel free to send inquiry, and you will get a quick reply. Look forward to cooperating with any willing purchaser.
Grade Performance | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni35 | Cr20Ni30 | |
Main chemical elements | Ni | rest | rest | 55.0~61.0 | 34.0~37.0 | 30.0~34.0 |
Cr | 20.0~23.0 | 28.2~31.0 | 15.0~18.0 | 18.0~21.0 | 18.0~21.0 | |
Fe | ≤1.0 | ≤1.0 | rest | rest | rest | |
Using temperature (max) ºC | 1200 | 1250 | 1150 | 1100 | 1100 | |
Melding point ºC | 1400 | 1380 | 1390 | 1390 | 1390 | |
Density g/cm 3 | 8.40 | 8.10 | 8.20 | 7.90 | 7.90 | |
Resistivity μΩ@m, 20 ºC | 1.09±0.05 | 1.18±0.05 | 1.11±0.05 | 1.04±0.05 | 1.04±0.05 | |
Ductility% | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | |
Specific heat J/g.ºC | 0.440 | 0.461 | 0.494 | 0.500 | 0.500 | |
Thermal conductivity KJ/m.h ºC | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
Coefficient of linear expansion a×10 -6ºC (20~1000 ºC ) | 18.0 | 17.0 | 17.0 | 19.0 | 19.0 | |
Microstructure | austenite | austenite | austenite | austenite | austenite | |
Magnetism | non magnetic | non magnetic | non magnetic | trace | trace |