PS plate Execution standards:
Coil line industry standard: HG/T2694-95
Reproduce plate industry standard: CY-T32-1999
PS plate type and character as follows:
Type | Base density | Character | Purpose |
GP | 0.27 | High-quality Al. base plate | High quality fine color printing |
HP | 0.27 | Moderate sand | Common printing |
QP | 0.15 | Moderate | Light printing plate |
YP | 0.27 | Even base | Sample plate |
PS plate specitation:
Common PS plate specification( base thickness 0.27) | ||||||||||
w | 960 | 1030 | 1030 | 920 | 905 | 810 | 810 | 680 | 650 |
|
L | 1220 | 820 | 770 | 760 | 565 | 594 | 577 | 640 | 550 |
|
Can be cut into different specifacations according to client’s demand (w<1050mm
Light printing plate specification (AL. plate thickness 0.15mm) | ||||||||
W | 100 | 115 | 320 | 395 | 360 | 395 | 365 |
|
L | 240 | 210 | 480 | 470 | 490 | 460 | 450 |
|
PS Plate reproduce
Huaxing company owns one prosuct line which can be produce single sheet, and also can be peodue and reproduce . repeosuce speification can be produce quarter plate , half plate and full plate etc.
Plate exposure:
Light source:
Huaxing PS plate can be exposed with HP mercury lamp, pulse xenon lamp, iodine-gallium lamp. But the best chioce is iodine-gallium lamp.
Exposure time: the base is gray gradient with 0.15 density difference. After 3rd grade grallium exposition, the sensitive layer is clean basically, and no-inking is the best exposure.
Exposure-time value for reference:
5000w iodine-gallium lamp distance 1.2m time 30-50s
3000w iodine-gallium lamp distance 1.2m time 70-100s
2000w iodine-gallium lamp distance 1.0m time 90-140s
Developing:
The Huaxing PS plate will used special developing powder, either machine or manually developing. Besides, other alkalescence developing liquids are also avaiable..
Usage:dissolve each bag powder with 5L warm warter into concentrated liquid, then fill water to dilute to 20L . then you can use immediately. The concentrated liquid and dilute liquid will be storage and seal.
Developing temperature:
The developing temperature is very important. The higher temperature will make PS Plate lose networks, of course, the printing ability will lower. Otherwise, the developing ability will be too low to develop well, and also the plate is prone to getting dirty. So proper developing temperature is normally at 20-25C. The developing time can not exceed 60s.
PS plate storage:
Taking PS plate will be done under yellow light. And also be escape from sunlight. The storage place should be dry , ventilative and cool. The shelf plate is one and half years.
factory introduce
Linyi Xinlong printing plate Meterial co.Ltd is located in Xinhua printing industrial park, a high and new technology developing zone in Shandong province, and it was established in 1994. Linyi Xinlong printing plate Co.Ltd. is a manufacture of new PS plates, which owns 4m single PS plate successive assembly-line and PS plate wrapping assembly-line. So it is capable to reproduce PS plate and produce high-quality PS plate. Therefore, the company can offer various specification of PS plate to meet your different demands. Moreover, our products are sold in more than 30 provinces and regions nationwide ,and also our products have good credibility.