AH36 shipbuilding steel sheet plate for sale
USD $500 - $700 /Ton
Min.Order:10 Tons
Shandong Jingen International Trading Co., Ltd.
AH36 Shipbuilding steel plate
Specification
Ah36 steel plate is used for shipbuiling&platform.The shipbuilding steel plate grade AH36 is the high tensile strength steel. Ah36 shipbuilding steel has good toughness properties, higher strength, strong corrosion-resistance, the processing properties, and welding properties. ASTM A131 Ah36 steel plate can be used in the manufacture of the ship's hull structure whose weight is more than 10000 tons.
AH36Shipbuilding steel plate specification:
Thickness: 4mm to 260mm,
Width: 1200mm to 4000mm
Length: 3000mm to 18000mm.
Chemical Composition % of Ah36 shipbuilding steel plate
| C | Si | Mn | P | S | Als | Ti | Cu | Cr | Ni | Mo |
AH36 | 0.18 | 0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |
Note: Generally speaking CE will be ≤ 0.40%. If the delivery condition is TMPC, the CE will be : ≤ 0.36% (thickness ≤ 50mm),≤0.38%( when the thickness >50-100). Ceq% =(C+Mn)/6+(Cr+Mo+V)/5+(Ni+Cu)/15.
Mechanical Property of Ah36 shipbuilding steel plate
| Rm | Re(MPa) min | A% min | Akv/J min | ||||||
AH36 | 440-570 | 315 | 22 | E.T °C | Thickness (mm) | |||||
0 | ≤ 50 | >50-70 | >70-100 | |||||||
L | C | L | C | L | C | |||||
31 | 22 | 38 | 26 | 46 | 31 |
Note: In the list , Rm: .tensile strength,Re: Yield strength,A%: elongation, E.T: experimental temperature,L: lengthways, C: crosswise.
Delivery Condition of Ah36 shipbuilding steel plate
| Fine grains elements | category | The thickness of steel | |||||
≤ 12 | >12.5-20 | >20-25 | >25-35 | >35-50 | >50-100 | |||
AH36 | Nb+V or V | Plate/ | A(50) | N(50),CR(50),TM(50) | N(50),CR(25),TM(50) | |||
Profile steel | N(50),CR(50),TM(50),AR*(25) | - | ||||||
Al or Al+Ti | Plate/ | A(50) | AR*(25) | - | ||||
N(50),CR(50),TM(50) | N(50),CR(25),TM(50) | |||||||
Profile steel | A(50) | N(50),CR(50),TM(50),AR*(25) | - |
Note: 1. delivery condition: A =Any ; N=Normalized ; CR=Control Rolled ; TM=TMPC, Temperature - deformation control rolling; AR*= Can be hot rolled with the agreement of Classification Society ; CR*=Can be control rolled with the agreement of Classification Society .
2. The Figure in the ( ) means the sampling volume to do the impact test, the unit is Ton.(-) means without impact test.
Contrast in the different standard
| TOCT 5521 | JIS G3106 | BS LR | GB712 |
AH36 | A36 | SM490B | AH36 | A36 |