Martensite stainless steel 440C Hot rolled annealed descaled sheared sheet

Martensite stainless steel 440C Hot rolled annealed descaled sheared sheet

Negotiable /Metric Ton

Min.Order:1 Metric Ton

Supply Ability:
500 Metric Ton / Metric Tons per Month
Port:
Shanghai
Payment Terms:
T/T

Quick Details View All >

Brand Name:
Changjiang
Model Number:
440C
Certification:
SGS
Length:
2000mm, or upon request, cut to length, straightened
Thickness:
3.0 - 16.0mm
Type:
Plate

Ahonest Changjiang Stainless Steel Co., Ltd. (Wuxi)

Business Type: Manufacturer,Trading Company
Wuxi Jiangsu China
Main Products: martensitic stainless hot and cold rolled strips ,special tool steels ,stainless steel strips in coils ,knife steels ,440C 440B 440A 420 1.4037 1.4034 1.4031 1.4028 1.4021 410 1.4116 1.4117 1.4419 1.4110 1.4120 1.4122 1.4923 1.4000 1.4003 1.2379..

Product Details

                                       

Martensite stainless steel 440C Hot rolled annealed descaled sheared sheet

 

Designations 

ChinaUSAJapanGermanyAustralia

GB 9Cr18

9Cr18Mo

9Cr18MoV

11Cr17

AISI 440C

UNS S44004

JIS SUS440C

EN 1.4125

DIN X105CrMo17

AS2837 - 1986 440C

 

Description

440C is a high-carbon chromium steel designed to provide stainless properties with maximum hardness.

440C stainless steel provides very good wear resistance combined with moderate corrosion resistance in mild environments.

440C is heat treatable to RC 59. This grade is commonly used in cutlery and food processing applications.

 

Chemistry data ( in weight % )

GradeCSiMnPSCrMoV
440C0.95 - 1.201.00 max1.00 max0.040 max0.030 max16.00 - 18.000.75 max-

 

Delivery state 

Annealed

 

Applications

Suitable for applications requiring a combination of excellent wear resistance with moderate corrosion resistance.

440C is commonly used in the oil and gas, marine, food and medical industries.

Typical applications are knives, scissors, surgical tools, cutlery, bearings etc.

 

Physical data

Specific Gravity   7.7 g/cm3

Density    0.28 lb/in.3

 

Heat treatment

Annealing

For maximum softness, this steel should be heated uniformly to 1550/1600°F (843/871°c).

Soak and cool very slowly in the furnace. Brinell hardness approximately 223.

Intermediate or process annealing treatment-heat uniformly to 1350/1400°F (732/760°c).

Air cool. Brinell hardness about 255.

 

Hardening

Heat to 1850/1950°F (1010/1066°c); soak; quench in warm oil or cool in air. Do not overheat.

When overheated, full hardness cannot be obtained. See comments under corrosion resistance.

 

Tempering

Hardness of approximately Rockwell C 60 will be obtained. To remove peak stresses and yet retain

maximum hardness, temper at least one hour at 300/350°F (149/177°c).

 

We are looking forward to your enquiries.

Contact:LIU

Email: sales@ahoneststeel.com

Cell:0086 18915272882

Contact Supplier

Ms. XINYING LIU Sales Manager Chat Now
Telephone
0086-510-83633959
Mobile
18915272882
Fax
0086-510-83633956
Address
No.520, Flat 4, Eastern Steel City, Xishan, Wuxi,Jiangsu

You May Like

New Products

Recommended Products

View More View Less

Find Similar Products By Category

Minerals & Metallurgy > Steel > Stainless Steel > Stainless Steel Sheets
Categories
Hi~