Green electrophoresis painting line/machine/system
USD $1 - $100,000 /Set
Min.Order:1 Set
Yangzhou Ours Machinery Co., Ltd.
Operating principle:
Putting the workpieces and corresponding electrode into the water-soluble paint and connecting the electricity supply. The resin and fillers in the paint will separate out equably on the surfaces of the workpieces and deposit to form water-fast paint films on the physical and chemical effects of electric fields.
Main parts of the full line:
1. Pretreatment device
2. Electrophoretic tank system
3. Electrophoretic transferring tank system
4. Stirring apparatus
5. Filter system
6. Water washing system
7. Ultrafiltration system
Parameters:
No. | Item | Description |
1 | Voltage | Iron and steel: 40~70V;Aluminum: 60~100V;Zinc: 70~85V |
2 | Electrophoresis time | 1~3 min for normal workpieces,3~4 min for large workpieces |
3 | Temperature of paint | 15~30 degrees |
4 | PH value of paint | 7.5~8.5 |
5 | Distance between the workpieces and the cathode | More than 20 cm |