fire resistant brick for fused cast skid rails block for hot steel reheating furnace
USD $3,200 - $5,000 /Ton
Min.Order:1 Ton
Zhengzhou Sunrise Refractory Co., Ltd.
Wear-Resistance bricks are made of raw materials such as high-grade bauxite and Australia imported zircon sand, which are melted and founded in high temperature electric furnace. It is mainly used in areas that require high abrasion and temperature resistance, such as gliding rail bricks in steel pusher metallurgical furnaces, the tapping platform (tapping spout) for tapping platform (tapping spout) style walking beam furnaces, and also as the interior for destructors.
Physical and chemical index:
Item | Behaviors TY-GM5 | |||
Special | Typical | |||
Chemical Composition % | Al2O3 | 71-74 | 73 | |
ZrO2 | 4.5-6 | 5.5 | ||
SiO2 | 17-20 | 19 | ||
Fe2O3 | ≤0.5 | 0.5 | ||
Na2O | ≤1.0 | 1.0 | ||
CaO | ≤0.5 | 0.5 | ||
Apparent Prosity (%) | 5-8 | <8 | ||
True density g/cm3 | ≥3.0 | 3.54 | ||
Cold Crushing Strength Mpa | ≥250 | 350 | ||
Hot Crushing Strength 1300°C Mpa |
| 45 | ||
Line Expansion 1150°C % |
| 0.9 | ||
Thermal conductivity 1250 °C: W/MK |
| 4.6 | ||
Bulk Density (g/cm3) | PT(RN) |
| ≥3.0 | |
WS(VF) |
| ≥3.2 | ||
Crystallographic analysis % | Corundum | 39 | ||
Mullite | 41 | |||
Glass Phase | 15 | |||
Baddeleyite | 5 |