ASTM B517 Inconel 600 Tube
Negotiable /Kilogram
Min.Order:50 Kilograms
Shanghai Chonray Precision Alloy Co., Ltd.
The picture of ASTM B517 Inconel 600 tube
600
Inconel 600 is a nickel-base alloy with excellent carburization, and good oxidation resistance at elevated temperatures. The alloy is widely used in the heat treating industry. 600 alloy has useful resistance to dry Cl2 and HCl gases at moderately elevated temperatures. Alloy 600 is not suggested for use at red heat when sulfur is present due to elevated nickel quantities.
Grades 200 and 201 nickel are normally preferred for handling concentrated, high temperature caustic. However, when sulfur compounds are present as well, or for ammonium hydroxide service, 600 alloy is suggested. 600 alloy is subject to stress corrosion cracking in hot, concentrated caustic alkalies. To avoid stress corrosion cracking, the 600 alloy fabrication should be fully stress relieved prior to use. A minimum treatment of 1650°F for 1 hour is suggested, but 1800-1850°F for 1 hour preferred.
Chemistry
| Ni | Cr | C | Mn | Cu | Si | S | Fe |
MIN | 72.00 | 14.00 | -- | -- | -- | -- | -- | 6.00 |
MAX |
| 17.00 | 0.15 | 1.00 | 0.50 | 0.50 | 0.015 | 10.00 |
Alloy form
Plate, rod , sheet, welding products
Common trade names
Alloy 600, Inconel 600, Nickel 600
Features
Applications
Physical properties
Density: 0.304 lb/in3
Melting Point: 2470- 2575°F
Poisson's Ratio: 0.29
Electrical Resistivity: 620 Ohm-circ mil/ft
Temperature, °F | 70 | 1000 | 1200 | 1400 | 1600 | 2000 |
Coefficient* of thermal expansion, in/in°F x 10-6 | - | 8.4 | 8.6 | 8.7 | 9.1 | 9.3 |
Thermal conductivity | 8.6 | 13.2 | 14.3 | 13.0 | 16.7 | - |
Modulus of elasticity, dynamic psi x 106 | 30.0 | 25.6 | 24.5 | 23.6 | 22.2 | 20.4 |
* 70°F to indicated temperature.
Mechanical properties
Representative tensile properties
Temperature,°F | 70 | 1000 | 1200 | 1400 | 1600 | 1800 |
Ultimate tensile strength, ksi | 93 | 84 | 65 | 27.5 | 15 | 7.5 |
0.2% yield strength, ksi | 37 | 28.5 | 26.5 | 17 | 9.0 | 4.0 |
Charpy impact V-notch, ft-lbs | 45 | 47 | 39 | 46 | 80 | 118 |
Static corrosion in molten caustic soda
Corrosion rate, mils per year
Temperature, °F | 750 | 932 | 1076 | 1256 |
Alloy 201 | 0.9 | 1.3 | 2.5 | 37.8 |
Alloy 400 | 1.8 | 5.1 | 17.6 | - |
Alloy 600 | 1.1 | 2.4 | 5.1 | 66.4 |
More products for you to choose.
Production line
Testing Equipment
Certification
Packing picture:
Our market
Our advantages and services
a. Our advantage
We can provide high quality material, excellent design, precise manufacturing,complete specifications, considerate and integrity serivices.
We can provide all kinds of electric heating alloy material and elements, including customized products.
We can provide a complete solution for you.
OEM service can be provided.
b. Technical services we can provide:
Product selection
Process optimization
New product development
Contact information: