Ground Coat Enamel Frits
Negotiable
Min.Order:1
Ground Coat and One-coat Enamel Frits | ||||
Reference No. | Description | Expansion | Firing | Application |
Coefficient (10-7) | Temperature (°C) | |||
UNG-102 | High Temp.Nickel Ground Coat | 301.8 | 840-880 | |
UNG-103 | High Temp.Nickel Ground Coat | 286.5 | 860-890 | |
UNG-104 | High Temp.Nickel Ground Coat | 290.1 | 840-880 | |
UNG-105 | High Temp. Antimony Molybdenum White Ground Coat | 297.1 | 840-870 | |
UNG-111 | Medium Temp.Co-Ni Ground Coat | 313.7 | 800-840 | |
UNG-112 | Medium Temp.Co-Ni Ground Coat | 292.1 | 820-860 | |
UNG-118 | Medium Temp.Nickel Ground Coat | 309.1 | 800-840 | |
UNG-124 | Low Temp. Antimony Molybdenum White Ground Coat | 290.1 | 780-820 | |
UNG-1102 | High Temp.Co-Ni Ground Coat | 300.5 | 840-880 | |
UNG-1112 | Medium Temp.Co-Ni Ground Coat | 283.6 | 830-860 | |
UNG-1122 | Low temp.Co-Ni Ground coat | 300.5 | 780-820 | |
UNG-2400 | Low Temp.Co-Ni Ground Coat | 322.1 | 760-800 | |
UNG-2401 | Medium temp.Co-Ni Ground Coat | 292.1 | 800-840 | |
UNG-2404 | High Temp.Co-Ni Ground Coat | 290.1 | 840-870 | |
UNG-2405 | High Yemp.Co-Ni Ground Coat | 288.1 | 860-880 | |
UNG-2406 | Temp. Resistant Co-Ni Ground Coat | 278.2 | 860-900 | |
UNG-2414 | Low Temp. Co-Ni Ground Coat | 311.1 | 760-800 | |
UNG-2115 | One-coat Black Enamel | 296.1 | 830-850 | |
Remarks: directly coated on base metal.with strong adherence. wide range of firing temperature. | ||||
1. Mill Addition Ratio for Nickel and Co-Ni Ground Coat: | ||||
Frit | 100 | Clay | 5-7 | |
Quartz porwder | 0-8 | Borax | 0.3-0.5 | |
Sodium Nitrite | 0.2-0.3 | Water | 50-55ml | |
2. Mill Addition Ratio of Sb-Mo Ground Coat: | ||||
Frit | 100 | Antimony Oxide | 1.0 | |
Clay | 5-7 | Barium Molybdate | 1.0 | |
Quartz Powder | 0-8 | Water | 50-55 ml | |
Frit Slurry Fineness | 1-2g/150mesh.100ml | Specific Gravity | 160-170g/100 ml |