Alloy 330 (UNS N08330)
Negotiable /Kilogram
Min.Order:50 Kilograms
Danyang HB Special Alloy Co.,Ltd
*Similar Grade
Trademark | UNS | W-Nr. |
Alloy 330 | N08330 | 1.4886 |
*Product Forms
Pipe, Tube, Sheet, Strip, Plate, Round Bar, Flat Bar, Forgings, Hexagon, Wire
*Brief
Alloy 330 (UNS N08330) is an austenitic nickel-iron-chromium alloy developed to provide excellent resistance to carburizing and oxidizing atmospheres at elevated temperatures. With a nickel content of 34 to 37 percent, the alloy remains highly resistant to both chloride stress corrosion cracking and embrittlement from the precipitation of sigma phase. It is readily fabricated using standard procedures for stainless steel and nickel alloys. The alloy is used extensively in elevated temperatures where resistance to the combined effects of thermal cycling and carburization is required.
*Chemical Composition,%
% | Ni | Cr | Fe | C | Mn | Si | P | S |
Min | 34.0 | 17.0 | Rest | 0.75 | ||||
Max | 37.0 | 20.0 | 0.08 | 2.00 | 1.50 | 0.03 | 0.03 |
*Typical Physical & Mechanical Property(Solution Annealed)
Density | Melting point | Tensile strength, MPa | Yield strength, MPa | Elongation,% |
8.08g/cm3 | 1380-1420℃ | 552-586 | 207-296 | 40-45 |
*Specification
Rod, Bar, Wire, Forgings | ASTM B536/ASME SB536 |
Plate, Sheet, Strip | ASTM B536/ASME SB536 |
Others | ASTM B366/ASME SB366(Fittings) |
*Feature
1. Corrosion Resistance
2. Alloy 330 provides a high level of corrosion resistance, particularly to oxidation, carburization, and nitridation. In aqueous environments the chromium content of 330 provides resistance to oxidizing conditions, while the nickel content enhances resistance to reducing conditions. The alloy’s high nickel content also makes it highly resistant to chloride stress corrosion cracking and sigma phase embrittlement.
3. Oxidation Resistance
4. Alloy 330 has good oxidation resistance and resists scale formation up to about 2000°F (1095°C). Any scale which is formed is tightly adherent, particularly under cyclic conditions of heating and cooling.
5. Carburization Resistance
6. The alloy's 35 percent nickel content and silicon addition contribute greatly to its excellent resistance to carburization. In alternating carburizing and oxidizing atmospheres, Alloy 330 exhibits excellent resistance to the ‘green rot’ phenomenon.
7. Nitridation Resistance
8. Alloy 330 exhibits good resistance to nitrogen-containing atmospheres where the oxygen content is low. It is used extensively in components handling cracked ammonia.
*Application
1. Chemical and Petrochemical Processing
2. Cracked ammonia components
3. Petrochemical furnace parts
4. Petrochemical waste remediation units
5. Heat exchangers
6. Flares
7. Ore Processing
8. Perlite systems and equipment
9. Power Generation
10. Boiler fixtures
11. Gas turbine components
12. Thermal Processing
13. Heat-treat furnace containers
14. Heat-treat furnace components
15. High temperature fans
16. Salt pots