Huawei Steel Ball ( ASTM E18,ISO 9001:2000)
Negotiable /Piece
Min.Order:10 Pieces
Huawei (Boxing) Machinery Manufacturing Co., Ltd.
HUAWEI Steel Balls
1. Chemical Composition
Name |
Chemical Composition (%) |
||||||
C |
Si |
Mn |
Cr |
P |
S |
Mo,Al,Cu,Ni,Nb,Ti,Zr,V,B,Mg |
|
High Chrome Alloyed Casting Ball |
1.8-3.2 |
0.3-1.2 |
0.3-1.0 |
10.0-10.5 |
≤0.1 |
≤0.1 |
Trace |
Low Chrome Alloyed Casting Ball |
2.0-3.5 |
≤1.2 |
≤1.0 |
0.5-1.5 |
≤0.15 |
≤0.25 |
Trace |
High Chrome Alloyed Casting Micro-Ball |
1.8-3.3 |
0.3-1.2 |
0.3-1.0 |
10.0-10.5 |
≤0.1 |
≤0.1 |
Trace |
Low Chrome Alloyed Casting Micro-Ball |
2.0-3.3 |
≤1.2 |
≤1.0 |
0.5-1.0 |
≤0.25 |
≤0.15 |
Trace |
2. Machanical Properties
Name
|
Machanical Properties |
||||
Specification |
Surface Hardness
|
AK (J/cm) |
Microstructure |
Times of Falling Balls |
|
High Chrome Alloyed Casting Ball |
Φ30-Φ130 |
58-66 |
≥2.5 |
M + C |
≥10000 |
Low Chrome Alloyed Casting Ball |
Φ30-Φ130 |
≥45 |
≥1.6 |
P + C |
≥8000 |
High Chrome Alloyed Casting Micro-Ball |
Φ8-Φ25 |
58-66 |
≥2.5 |
M + C |
≥10000 |
Low Chrome Alloyed Casting Micro-Ball |
Φ8-Φ25 |
≥45 |
≥1.6 |
P + C |
≥10000 |
3.PLC Production Line
The most advanced PLC Automatic Control Casting Production Line is specific to the production of diameter 8mm-40mm micro-balls with high efficiency, stable quality and low flaw.
4.Heat Treatment
The domestic first MCGS uniform temerature graduation oil-quenched production line,uses the computer long-distance visualization control.The temperature and the oil temperature carry on the accuracy control to the stove. Guarantee quenching quality maximum limit.Hardness of product high chromium cast grinding ball is bigger than HRC 62.The difference of surface hardness and centre hardness is less than 2 HRC. Residual Austenite less than or equal to 5%, Martensite organization of thin strip.Application of ball consumption of less than or equal to 20g/ton.
5.Medium Frequency Induction Furnace
The medium frequency induction furnace we applied was developed by the Xi'an Jiaotong University, using 660V low-voltage power transmission, by improving the frequency power supply and control voltage current value , the maximum extent has accelerated the melting speed. Improve efficiency, reduce the burning of alloy elements, ensure the stability of the material.
6.Laboratory
We have a wear-resistant materials, provincial qualified R & D Center, consists of microscopic detection room and the physical and chemical examination room, with the most advanced spark –direct reading spectrometer in the country, ultrasonic flaw detector, metallography microscope, universal material testing machine, drop ball testing machine and other testing equipment the maximum guarantee product quality and new product development.