307 Light Weight Polyester Putty
Negotiable /Metric Ton
Min.Order:1 Metric Ton
Foshan Shunde Himens Industrial CO.,Ltd
307 Light Weight Polyester Putty
Ingredients:
Unsaturated polyesters resins, modified resin, color pigment, stuffing, anti sediment materials, auxiliary agent and firming agent mixing ratio 100:2.
Characteristics:
The ash is exquisite and has excellent construction performance, which can well tamp the sand holes left after rough scraping with polyester putty. Also, polyester putty finely scraped enjoys quick drying, good sanding property and adhesion. It is mainly applicable to the filling and leveling up as well as decoration of the deficiencies such as sand holes, pinholes and shrink holes on the surface of polyester putty before closing the undercoat in the painting dressing of cars, so as to strengthen the flatness and smoothness of the surface of polyester putty. And it meets the requirements of flatness and smoothness etc. on the appearance of top coating.
Main technical standard:
Item |
Index |
Testing Standard |
Outward appearance |
The color is unanimous, and there are no visible particles by naked eye, and being rather exquisite |
Visual examination |
Air drying |
Meet the customers requirements |
GB/T1728-79 |
Consistency |
9-12cm (except for the specialities) |
GB/T1749 |
Scratching performance |
Good handling, no curling |
|
Burnishing performance |
Burnishing easy, extraction powder is fast. |
|
Resistance to high temperature |
There is no bubbling and cracking under baking at 120 degree centigrade after drying |
|
There is no bubbling and cracking under baking at 80 degree centigrade after gelling |
|
|
Pliability |
Less than 50mm |
GB/T1748 |
Impact Strength |
More than 15kg.cm (or 35kg.cm Not falling off) |
GB/T1732 |
Adhesive force |
More than 50Kg/1.2cm2 |
GB/T5210 |
Reference for construction:
1. Evenly mix the main ash and firming agent with the proportion being 100:2 (make the color unanimous), and using up them within the gelation time.
2. Scratch the putty which has already finely mixed on the primer paint of double components after burnishing or the surface of cold-rolled sheet which has already been finished processing. If the thickly scratching is required, you had better thinly scratch for many times to meet the required thickness. If some air bubbles infiltrate while scratching, you should thoroughly strickle it by means of scraper, so as to ensure the good adhesive force. The best wet milling time is 0.5-1h after scratching.2-3h is the best dry milling time.
Notes:
1. Once the putty mix firming agent, don’t put it into can and cover it after using in case that the impregnant volatilization may result in the deterioration of main ash.
2.The solidifying period of coating film will extend if the temperature is high or low. The consistence and gelation time of putty may adjust according to the requirements of customers.
3.This product is unsuitable for directly scratching on galvanization plates.
4. Its quality can be guaranteed for 6 months since the date of its production. I(f it does not beyond this period, it can be used continuously).