CNC Machined Fabricated Molybdenum Parts / MolyProducts For Vacuum Furnace
USD $4 - $5 /Piece
Min.Order:1 Piece
Hubei Fotma Machinery Co., Ltd.
99.95% Pure Tungsten Products Tungsten Crucibles dia 10 - 500 mm for Sapphire
YG8 / YG10 Tungsten Carbide Cutting Tools , Ground Tungsten Carbide Blade for Paper Cutter
Customized Mechanical Tungsten Carbide Wear Parts Seal Rings for oil and gas industry
CNMG DNMG Tungsten Carbide Cutting Tools , TiN Coated Tungsten Carbide Products
SEKN SPAN TPAN Tungsten Carbide Cutting Tools CNC Carbide Milling Inserts C2 C5
LNE LNR YCE Tungsten Carbide Tooling Products Heavy Duty CNC Cutting Inserts
CNC Machined Molybdenum Products Molybdenum Fabricated Parts For Vacuum Furnace
Molybdenum has outstanding electrical and heat-conducting capabilities and relatively high tensile strength. Thermal conductivity is approximately 50% higher than that of steel, iron or nickel alloys. It consequently finds wide usage as heatsinks. Its electrical conductivity is the highest of all refractory metals, about one third that of copper, but higher than nickel, platinum, or mercury. The coefficient of thermal expansion of molybdenum plots almost linearly with temperature over a wide range. This characteristic, in combination will raise heat-conducting capabilities, accounts for its use in bimetal thermocouples. Methods of doping molybdenum powder with potassium aluminosilicate to obtain a non-sag microstructure comparable to that of tungsten also have been developed.
Molybdenum Parts Applications:
Machinery / Medical / Auto / Solar / LED / Motor / Electrical / Electronic/
Sensor / Automation Equipment / Lock / Communication / Plumbing/
Laser / Aerospace / Building Facilities / Sports Facilities / Computer/
Office Equipment / Precise instrument / Automobile Engine / Printing/
(Fax Machine/ Copying Machine / Printer / KMKZ) / Loom /
Sewing Machine / Elasticizer/ drawing frame / combing machine
Comparation of Tungsten and Molybdenum:
Molybdenum |
Tungsten |
||
Density |
G/CM3 |
10.22 |
19.3 |
Melting point |
oC |
2620 |
3410 |
Thermal conductivity |
W/M.K |
98.8 (1400 oC ) |
174 (10--100 oC ) |
Resistivity |
Ω.CM |
53.1 (1730 oC ) |
35 (1000 oC ) |
Vapor pressure |
Pa |
7.09 X 10-6 (1600 oC ) |
low |
Modulus |
/MPa |
343 350 |
35 316 |
Thermal expansion coefficient |
K-1 |
6.2 X 10-6 (700 oC ) |
4.5 X 10-6 (0--100 oC ) |
Hardness |
HB |
35--125 |
290--350 |
Tensile strength |
MPa |
687 |
981-1472 |