1.Surface Treatment: As the customers' requests
2.Standard:ASTM
3.Good quality and low price
We supply this grade in the following forms: Bar, wire, sheet, plate, coil, fasteners and forgings.
INCONEL 718 has excellent mechanical properties at elevated temperatures, as well as cryogenic temperatures. Suitable for temperatures upto around 700°C.Applications include gas turbines, rocket motors, space craft, nuclear reactors and pumps.
Typical analysis in percent
Cr |
Ni |
Mo |
Co |
Cb+Ta |
Ti |
Al |
Fe |
19 |
52.5 |
3.05 |
1 max |
5.13 |
0.9 |
0.5 |
18.5 |
Physical properties
Density: 8.4g/cm3
Melting range:2350-2460°C
Typical mechanical properties(At room temperature)
Ultimate tensile strength(mpa) |
Yield strength(mpa) |
Elongation in 50 mm(%) |
1275 |
1034 |
12 |