16 Gauge Construction and Building Reinforce Galvanized Iron Binding Wire
1. Galvanized Iron Binding Wire details
a. 16 Gauge Binding Wire
b. Zinc coating: 7-18g/m2
c. Tensile Strength:30-70kg/mm2
d. Elongation Rate: 10%-25%
e. Weight:0.1-800kg/coil
2. The Construction and Building Binding Wire making process of hot dipped and electro galvanized wire
Iron wire rod→Wire Drawing→Wire Annealing→Rust removing→Acid Washing→Zinc coating→Wire Coiling → packing
First : careful control from steel rod coil .
Sencond:iron wire rod drawing,then the iron wire rod turn the dia you need.
Third :annealing ,we get the black iron wire .
Fourth :rust removing , we use Anti-rust oil ,not Waste engine oil .Then we got black annealed iron wire
others:acid washing ,boiling ,drying ,zinc feeding to wire coating
At last:we get the electro galvanized steel wire/hot dipped galvanized steel.
3.Contact Me: