Hot sale popular 20 gauge binding wire galvanized iron wire
USD $490 - $500 /Ton
Min.Order:100 Tons
Hebei Xun Qiang Wire Mesh Products Co., Ltd.
Hot sale popular 20 gauge binding wire galvanized iron wire
galvanized iron wire is made by Q195 mild stee wire rod . Main process is wire drawing , achid washing , rust removing , annealing , zinc coaing , coiling and packing . Mainly used in construction , handocraft , woven wire mesh , express way fencing mesh , packaging of products and other daily uses .
Specifications:
1 . Mateiral : Q195 Low Carbon Steel Wire
2 . Zinc coating : 40-230g/mm2
3 . Tensile strength : 350--550 N
4 . Elongation : 10%
5 . Coil weight : 25 kg , 50 kg , 100 kg , 500 kg
Features :
1. Excellent flexibility and softness
2. Suitable usage : woven wire mesh , binding wire , making hangers and so on .
Mobile: 0086-15610971700
SKYPE: xunqiang6| WhatsApp: 15610971700 | Wechat: 591814752 | Web:
Raw material
------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------
Q195 wire rod---this type of wire rod has less impurities so it very suit for drawing. Q195 material's chemical component is nearly same as SAE1008 and SAE 1006. Q195 material chemical component :
C≤0.07; S≤0.023; Si≤0.09; Mn≤0.32; P≤0.025.
Galvanized wire production process
------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------
1 . Galvanized wire’s first stage is drawing
there are two kinds of drawing machine: powder drawing and water drawing. powder drawing is fit for juniordrawing(6.5mm~4.0mm). One powder drawing machine has 4 tanks and 4 molds. One tank is matched with a mold. Each of them are offered energy by a electromotor. 0.9mm(max)can be “eat” when the wire cross a mold. There are no loss of weight during drawing.
2 . Galvanized wire’s second stage is annealed
Anneal is to low the tensile strength of wire . The stove is solid and built with red bricks. The architecture of anneal stove is cuboid . Different thickness of wire require different temperature . Range is from 700℃to 900℃ . Output of the anneal stove , the tensile strength is 400N~500N .
3 . Galvanized wire’s third stage is chlorhydric acid washing
After the draw and anneal, the wire is thinner, softer but also much more dirty. It needs chlorhydric acid washing to remove the impurities. Chlorhydric acid washing requires water pool and chlorhydric acid pool. The density of chlorhydric acid is 17%. In the Chlorhydric acid pool, there is a caldron used for the emission of vapor.
Electro galvanized is a chemical reaction. One chlorhydric acid pool is enough. However, hot-dipped is a physical reaction, it needs two chlorhydric acid pool and two water pool for the preparation of galvanization.
4 . Galvanized wire’s fourth stage: Zinc coating
After the chlorhydric acid pool, water pool is also necessary. In the zinc pool, displacement reaction is chemical and uniformly distributed. The surface of wire is smooth. Because wire cross the zinc pool fast, abundant zinc coating requires 4 zinc pools.
APPLICATIONS:
Extensively used in
Our team are professional maketing composed with power.We are young and capable with experience in different sectors of international trade promote an atmosphere of openness,respect and trust,bringing a sense of teamwork,collegiality and diversity to all we do.In order to our dream,we try our best and persistence,even meet big risk,we also believe that we are the best.
Through it all,we develop strong relationship with each other and we have built long term relationship with our customers.