Antifreeze agent for concrete water reducer
USD $180 - $250 /Metric Ton
Min.Order:20 Metric Tons
Hebei Shengtong Building Materials Technology Co., Ltd.
ST-01C High Performance Antifreeze include powder and liquid .By reduction of water, antifreeze and other components of a composite made of a composite antifreeze, the product content, good frost effect and enhance the effect. Chlorine-free, low-alkali, it can be widely applied in civil engineering, construction in winter mixing stations, highways, railways, water conservancy and hydropower and other large concrete projects.
Specification as below :
item | Specification | |||
Solid content(%) | 19.5-20.5 | |||
density(g/ml) | 1.00-1.04 | |||
Chloride content(%) | ≤0.10 | |||
Alkali content (%) | ≤8 | |||
Mud Fluidity(mm) | ≥210 | |||
Water Reduction(%) | ≥10 | |||
Ratio of bleeding rate (%) | ≤80 | |||
Containing gas (%) | ≥2.5 | |||
Setting time | Start setting (min) | -150~+150 | ||
Fianally setting (min) | -210~+210 | |||
Shrinkage ratio in 28 days (%) | ≤135 | |||
Penetration height ratio (%) | ≤100 | |||
Thaw strength loss rates than in 50 times (%) | ≤100 | |||
Steel corrosion effect | no | |||
Compressive strength ratio | Specifications Temperature (℃) | -5 | -10 | -15 |
R-7 | ≥20 | ≥12 | ≥10 | |
R28 | ≥100 | ≥95 | ||
R-7+28 | ≥95 | ≥90 | ≥85 |
1. Powder package: woven bags with plastic inner. specifications: 50kg ± 0.5kg / bag;
2.Transport: The product is non-flammable dangerous goods, car or train transportation available, during transport powder should be noted that anti-breaking damage, moisture, agent should pay attention to seal and waterproof.
3. Storage: Powder should be stored in ventilated, dry place, pay attention to prevent damage and moisture. After the performance the same damp, if knot blocks can be ground into a powder, does not affect results; agent in a cool dark place sealed, must not its he chemical product mix.
4.Validity: Under normal conditions, one year.
Use and Construction Notes
1.Recommended dosage (in cementitious materials basis) :
( 2.0 to 3.0)%: temperature (0 ~ -5) ℃
(3.0 to 3.5)%: temperature (-5 ~ -10) ℃
(3.5 to 4.0)%: temperature (-10 ~ -15) ℃
2. powder and binder directly into the mixer together with stirring, a liquid can be directly added to the mixer together with the mixing water the solution in the water mixing water should be deducted and extend the stirring time 30s
3. When the temperature is below -5 ℃, the water should be heated to 60 ℃, gravel must not be mixed with ice.
4. The incorporation of concrete this product should be used in mechanical stirring, and stirred no less than 3min.
5. concrete such as the mold temperature should be greater than 5 ℃, pouring is completed, the insulation material should be covered immediately to prevent dehydration.
wahtsapp id :008615511345298