Sharp design wet milling with high efficiency supplied by manufacture
USD $4,000 - $10,000 /Set
Min.Order:1 Set
Gongyi Dongxing Material Trade Co., Ltd.
1. About wet pan mill
The wet pan mill is a new mill, small investment, high yield, the production cost is low, good benefits.
2. which model is suitable?
The wet pan mill is named by the diameter of roller. Φ1300,Φ 1350,Φ 1400,Φ 1500,Φ 1600 is suitable for selection of iron ore, molybdenum ore ,lead ore ,zinc ore, antimony ore and so on. Φ 850, Φ 900, Φ 1000,Φ 1100,Φ 1200 is suitable for selection of gold ore.
3. Wet Pan Mill using scope
Mainly used with gold, silver, lead, zinc, iron, molybdenum, copper, antimony mine.
Model | Specification | Input size(mm) | Rotate Speed (r/min) | Powder(kw) | Weight(t) |
1600A | 1600×400×200×500±20mm | <30mm | 20-22 | 25KW | 14.5 |
1500A | 1500×350×200×460±20mm | 20-22 | 22KW | 13.5 | |
1500B | 1500×350×150×460±20mm | 20-22 | 22KW | 12.3 | |
1500C | 1500×300×150×420±20mm | 20-22 | 22KW | 11.3 | |
1400A | 1400×250×150×350±20mm | 16-18 | 18.5kw | 8.5 | |
1400B | 1400×250×150×350±20mm | 21-23 | 18.5kw | 8.5 | |
1350A | 1350×250×150×350±20mm | 16-18 | 18.5kw | 8 | |
1350B | 1350×250×150×350±20mm | 21-23 | 18.5kw | 8 | |
1300A | 1300×250×150×350±20mm | 16-18 | 15kw | 7.5 | |
1300B | 1300×250×150×350±20mm | 21-23 | 15kw | 7.5 | |
1200A | 1200×200×80×250±20mm | 17-19 | 7.5kw | 5.5 | |
1200B | 1200×200×80×250±20mm | 23-25 | 7.5kw | 5.5 | |
1100A | 1100×200×80×250±20mm | 17-19 | 7.5kw | 5 | |
1100B | 1100×200×80×250±20mm | 23-25 | 7.5kw | 5 | |
1000 | 1000×200×80×250±20mm | 13-15 | 5.5kw | 4.5 |
Wet Pan Machine Use and Maintenance:
ü The normal operation of the mill, before they start feeding.
ü This machine prohibit strip start, the outage at boot time, you must first clean up the residual ore in the middle of the milled slot and then start.
ü Should be uniform feeding not erratic, it is best to use the feeder Part.
ü Bearing frequent butter, gear box or car rear axle with frequent checks whether the loss of gear oil.
ü Regular checks of the various parts of the screw is loose.
ü Found bearing damage must be promptly replaced, shaft eccentric avoid damage to other parts
ü Mill runtime to pay attention to that the reducer or bearing part of the presence or absence of abnormal sound, whether the temperature is too high, the motor current is too large irregularities; should be shut down immediately if the above phenomenon, exclude.
ü Machine maintenance, to ensure safety, you must remove the motor belt.