UFR Powder
USD $1,000 - $1,500 /Metric Ton
Min.Order:10 Metric Tons
Henan Premtec Enterprise Corporation
A Product Speciality:
When use 202C Pure UF Resin Powder,users can apply different kind of additives according to the requirement (This should be under Technicians guidance). The user can process 202C pure UF Resin Powder to different wood adhesives according to their actual need. This Powder is suitable for the cold pressing and hot pressing project. The outstanding characteristic of 202C is strong adaptability and flexible construction conditions. The 202C Pure UF Resin Powder could mix with the general kind of hardeners and could reach normal bonding effect.
High bonding strength
Convenient for using
Formaldehyde emission could reach International standard
Both cold and hot solidification could reach ideal effect
Similar wood color, and do not pollute the wood
Excellent water-proof performance
Convenient for transportation
B Application Areas
202C is suitable for the processing of plywood, particle board, MDF&HDF, multi ply wood and the other wood production which need to use cold setting technology. Below are mainly applications for reference:
Various kind of artificial boards
Gluing Plywood & Bentwood
Surface veneer for door and decorative boards
Engineered solid wood flooring
Finger or butt joint of woods
C Performance Index
Item | Unit | Description |
Appearance |
| White Powder |
Moisture Content | % | ≤1 |
Cured Period (20) | Depend on the Added Qty of Hardener | |
Shearing StrengthUnder Pressure after 20h | Mpa | >15 |
Shearing Strength of Water Resistance Under Water after 24h | Mpa | >11 |
Active Period after Mixture | Depend on the Added Qty of Hardener |
D Usage Method:
1. Pretreatment for gluing wood material:
a) Moisture Content reach to 10 + 2%
b) Remove Knots, Cracks, oil stain and resin etc.
c) Wood surface must be flat and smooth. (Thickness Tolerance0.1mm
2. Mixture of Glue
a) Mixture Ratio(weight): UF Powder: Water=1: ≤0.6
b) Dissolution Method:
Put 2/3 of the total needed water into mixer, and then add UF powder in. Switch on the mixer with speed of 50~150 rotations / minute till to being completely dissolved.
Put the remained 1/3 water in mixer and churn about 3~5minutes till to being completely dissolved.
c) The user could add hardener into the mixed liquid glue depend on the actual requirement, and control workable period of dissolved liquid glue.
3. Gluing Operation:
1) Gluing Quantity: Depend on different wood material and working temperature. Generally, 2 sides sub is: 200~300g/m2.
2) Required Press Condition:
The pressure and Process Time depend on different wood species and process temperature. Please refer to below instruction:
Wood Species | Coniferious wood | Broad-leaved wood | ||
Temperature | 5-25 | >25 | 5-25 | >25 |
Gluing Qty(2 sides) (g/m²) | 200-250 | 250-300 | 200-250 | 250-300 |
Pressure (MPa) | 0.8-1.0 | 0.8-1.0 | 1.2-1.5 | 1.2-1.5 |
4. Maintenance:
After pressure relief, the glued board could be used on the second day. In winter, board must be maintained at least 12 hours under temperature above 20 before put into process.
5. Heat Solidification Operation:
The glued board with above mentioned pressure for 5~7minutes under temperature 100-110. It could be used after release of press.
E Note:
1. The goods should be stored in a dry, ventilated location. Avoid direct sunshine and moisture.
2. The package should be sealed again immediately once the pack of UF powder has been opened to avoid moisture.
3. Avoid contact with eye. Once splashed into eyes, flushed out with plenty of clean water. Consults doctor if necessary.