Refractory Insulation High temperature resistance Fire Brick
USD $1 - $3 /Piece
Min.Order:100 Pieces
Laizhou Sunshine Trading Co., Ltd.
Fireproof brick
Product usages
Used for building steel furnace, furnace refining furnace, non-ferrous metal smelting furnace, cement kiln, glass kiln, etc.
Production process
Production technology of calcined magnesite chrome brick and magnesite chrome bricks in line. In order to eliminate
the bricks in burning process because of MgO style and Cr2O3, Al2O3, or directly combined magnesite chrome
brick. The main raw material of manufacturing magnesite chrome brick is sintered magnesite and chromite. Magnesia raw material purity as high as possible, chromite
chemical composition requirement is: the Cr2O3:30 ~ 45%, CaO: 1.0 ~ 1.5% or less.
Classification
Brick according to the physical and chemical indicators divided into MGe - 20, MGe - 16, MGe - 12, MGe - 8 four grades
Refractory temperature: 1580 ~ 1770 °C (°C)
Technical index
Kind | direct-bonded magnesia-chrome bricks | semi-rebonded magnesite-chrome brick | ||||||||||
| MGe8A | MGe8B | MGe12A | MGe12B | MGe16A | MGe16B | MGe18A | MGe18B | MGe16A | MGe16B | MGe20A | MGe20B |
MgO % ≥ | 74 | 74 | 66 | 66 | 60 | 60 | 58 | 58 | 60 | 60 | 55 | 55 |
Cr2O3% ≥ | 8 | 8 | 12 | 12 | 16 | 16 | 18 | 18 | 16 | 16 | 20 | 20 |
SiO2 % ≤ | 1.5 | 2.0 | 1.5 | 2.0 | 1.5 | 2.0 | 1.5 | 2.0 | 1.5 | 1.8 | 1.5 | 1.8 |
apparent porosity% ≤ | 18 | 18 | 18 | 18 | 18 | 18 | 18 | 18 | 17 | 17 | 17 | 17 |
cold crushing strengthMPa ≥ | 40 | 35 | 40 | 35 | 40 | 35 | 40 | 35 | 40 | 35 | 40 | 35 |
Load softening point°C ≥ | 1660 | 1600 | 1660 | 1600 | 1660 | 1600 | 1660 | 1600 | 1750 | 1700 | 1750 | 1700 |
Photo