(N-TYPE)MADE IN TAIWAN ECO FRIENDLY PAINT RAL 5012 FOR LATHE MACHINE
USD $24.12 - $36.67 /Set
Min.Order:2 Sets
(N-TYPE) MADE IN TAIWAN RAL 3000 SPECIAL EFFECT PAINT SPRAY LACQUER
(N-TYPE) MADE IN TAIWAN CHROMATIC PANTONE SPRAY PAINT ENTERPRISE PAINTS
(N-TYPE) TAIWAN MADE ANTI FRICTION COATINGS 2K METALLIC BLACK PAINT
MADE IN TAIWAN EPOXY ANTI-RUST STAINLESS SPRAY PAINT BASECOAT
(N-TYPE) MADE IN TAIWAN ACRYLIC COATING ANTICORROSION METAL TEXTURE PAINT
(N-TYPE)MADE IN TAIWAN LIGHT GRAY RAL 7035 ASIAN PAINT ANTI ACID COATING
(N-TYPE)MADE IN TAIWAN ECO FRIENDLY PAINT RAL 5012 FOR LATHE MACHINE
POLYURETHANE COATING(N-TYPE) | |
TYPE | A two-pack, polyurethane finish enamel based on Acrylic Polyol, resins and non-yellowing Isocyanate Hardener with weather resistant pigments. |
USES | Top coat for vehicles, bridges, boot top, topside steel structures, and wooden and metal products, etc. |
CHARACTERISTICS | 1. High gloss with excellent appearance. 2. Excellent resistance to weathering with gloss retention. 3. Excellent resistance to oils, acids, alkalis and solvents. 4. Excellent hardness, adhesion and abrasion resistance. |
GLOSS | Above 90% |
COLOR | Desired colors |
WEIGHT | Above 1.0 kg/L (Mixer) |
VISCOSITY (25 °C) | 60– 85 KU (Mixer)(25 °C) |
DRYING TIME (25 °C) | Set-to-touch 1 hr. Dry hard 6 hrs. (25 °C). |
OPTIMUM FILM THICKNESS | Wet 95μ(microns)Dry 30μ(microns) |
MIXER RATIO | Base: Hardener = 2: 1 (by volume.) |
NON-VOLATILE CONTENT | Above 55% |
POT LIFE | 4 hrs. (Mixture , 25 °C) |
THINNER | PU Thinner |
THINNING RATE | 10~25 % |
STORAGE SHELF LIFE | Minimum 1 year under normal storage conditions. |
APPLICATION METHOD | Spray, Brush. |
NOTE | 1. Mix base and hardener according to the mixing ratio and stir thoroughly. 2. Avoid applying the paint in rain or humid weather, particularly, a wet surface must be thoroughly dried. 3. All equipments must be cleaned immediately after use. 4. When used inside tanks, sufficient ventilation must be provided. 5. When overcoating interval is exceeded, paint surface must be roughened to insure adhesion. 6. Hardener can must be tightly closed to avoid reaction with moisture in air toform bubbles and gelation. 7. Strictly controlling application, not be exceed 60μ pre coat, to avoid bubbles for mation. |