Carbonized Thermowood Solid Wood Decking
USD $20.5 - $22.5 /Square Meter
Min.Order:1200 Square Meters
Fujian Qin Chao Timber Technology Co., Ltd.
Grade: Pine (Redwood) Thermowood.
No worm holes, no rotting, no wane
Colour: The color of the thermowood changes due to caramelization of glucose inside the wood , Hemicellulose is separated into furfural and carboxylic acid. Caramelization of lignin, caused by heat, results in a darker color, so Thermowood has a rich brown colour.
When exposed to the UV light it will weather to a beautiful silvery grey colour, unless otherwise protected by a stain.
Description: Due to its stability and resistance to moisture and decay. Thermowood is an excellent choice of timber for both claddings and decking.
For further and full details on Thermowood please see our thermowood explaining.
* Please feel free to'ask any questions'Technical or Otherwise, Our Sales Team is here to Help.
Daisy---WhatsApp: +86-18650121916 Skype: daisy_2011916
Cover: 145mm - 10.20 linear metres cover 1m2.
120mm - 8.33 linear metres cover 1m2
95mm - 10.53 linear metres cover 1m2
Fixings: Secret fixed using 60mm stainless steel fixings - This profile should be fixed horizontally using 40mm stainless steel nails.
Lengths Available: Supplied in fixed lengths of 4M and 3M while4M is themain
In the event that you require specific selected lengths please contact us.
Price: Is per square meter.
If you are looking to purchase less than 1000m2 or more than 10000m2 please contact us for a quotation.
Fujian Qin Chao Timber Technology Co.,Ltd
1.How can the wood be thermally modified?
The process can be divided into three phases:
1. Temperature increase and high temperature drying:
Wood temperature is raised rapidly using heat and steam to a level of around 100 °C. In this phase we use steam because if the heat temperature of wood is too much this wood directly explored, so we need to use steam. In this phase the moisture become nearly to (%0).
2. Heat Treatment:
Whenever high heat drying is occurred the temperature is increased to a level of 185-215 °C. After we reach to that heat temperature with the type of wood (2-3) hour is remains in the same heat. In this phase the steam make the wood not burn.
3. Give the moisture to wood:
In the final stage, the temperature is reduced to 50°C-60 °C by using water spraying system, this process is continued to when the moisture content is reached to 4% -6%.
2.Why choose us and our thermowood?
3. Where can the Thermowood be used?
Thermo-S
The letter 'S' in 'Thermo-S' stands for 'stability'. Along with appearance, stability is a key property in the end user applications of the products in this treatment Class. The average tangential swelling and shrinkage due to moisture for Thermo-S class treated wood is 6–8%.
Thermo-S Soft Wood | Thermo-S Hard Wood: |
- Building Components | - Furnishing |
The letter 'D' in 'Thermo-D' stands for 'durability'. Along with appearance, Biological durability is a key property in the end user applications of products in this treatment class. The average tangential swelling and shrinkage due to moisture for Thermo-D class treated wood is 5–6%.
Thermo-D Softwood | Thermo-D Hardwood |
- cladding - outer doors - shutters - environmental constructions - sauna and bathroom furnishing - flooring - garden furniture | End user applications as in Thermo-S. If a darker color is desired, Thermo-D Should be used. |
4. Can I get some sample?
Yes, we can send you free samples, but the shipping cost should be on your side.
5. How can I get the sample?
5. Can you do my customized sizes?
Yes, give me your specification and design paper if possible, it will take 1-12 hours to quote depends.
6. How can I place the order?
Contact Daisy---WhatsApp +86 18650121916 Skype: daisy_2011916 EM: daisy_zhan at qinchaowood de com
or
Send me inquiry through website directly.