hdpe geomembrance dam liner
USD $0.32 - $3.56 /Square Meter
Min.Order:5000 Square Meters
Feicheng Haicheng Plastic Package Co., Ltd.
mechanical properties hdpe pond liner,flexible fish pond,hot sale hdpe geomembrane
non-toxic HDPE pond liner,high quality geomembrance, waterproof protection HDPE fish pond
anti-corrosion HDPE pond liner,hot sale various usage geomembrane
anti-oil and salt hdpe pond liner,0.85mm thickness Geomembrance,long service life fish pond
Feicheng Haicheng Plastic Package Co,.Ltd is a pe/pvc tarpaulin supplier in China. We can produce any waterproof cover as your requirement. HDPE geomembrance is a good dam ,pond liner etc. It is widely used in construction water conservation, environmental protection, traffic and tunnel ...
HDPE thickness is between 0.2mm and 3.0mm, width from 4m to 7m; LDPE thickness from 0.3mm to 3.0mm, width from 4m to 7m.
Features Specifications: HDPE Geomembrane
High Density Polyethylene(HDPE) Geomembrane
smooth
Properties | T est method | Test Value(ave.) | ||||||
0.50mm | 0.75 mm | 1.00mm | 1.25mm | 1.50mm | 2.00mm | 2.50mm | ||
Width(mm) | ______ | 7000 | 7000 | 7000 | 7000 | 7000 | 7000 | 7000 |
Thickness -mm (min. ave.) L owest individual of 10 values | ASTM D5199 | nom. -10% | nom. -10% | nom. -10% | nom. -10% | nom. -10% | nom. -10% | nom. -10% |
Density g/cc(min.) | ASTM D1505/D792 | 0.940 | 0.940 | 0.940 | 0.940 | 0.940 | 0.940 | 0.940 |
Tensile Properties: Y ield strength break strength Y ield elongation break elongation | ASTM D638 Type IV | 10N/mm 16 N/mm 15% 780% | 14N/mm 24 N/mm 15% 780% | 19N/mm 33N/mm 15% 780% | 24N/mm 41 N/mm 15% 780% | 29N/mm 50N/mm 15% 780% | 38N/mm 66 N/mm 15% 780% | 46N/mm 83 N/mm 15% 780% |
Tear Resistance-N | ASTM D1004 | 75 | 115 | 150 | 190 | 230 | 300 | 375 |
Puncture Resistance-N | ASTM D4833 | 240 | 360 | 480 | 590 | 680 | 840 | 950 |
Stress Crack Resistance | ASTM D5397(APP) | 300hr. | 300hr. | 300hr. | 300hr. | 300hr. | 300hr. | 300hr. |
Carbon Black Content-% | ASTM D1603 (3) | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% |
Carbon Black Dispersion | ASTM D5596 | note | note | note | note | note | note | note |
Oxidative Induction Time(OIT) (min. ave.) (a)Standard OIT or (b)High Pressure OIT | ASTM D3895 ASTM D5885 | 100min. 400min. | 100min. 400min. | 100min. 400min. | 100min. 400min. | 100min. 400min. | 100min. 400min. | 100min. 400min. |
Oven Age at 8 5 Standard OIT (min.ave.)-%retained after 90 days | ASTM D5721 ASTM D3895 | 55% | 55% | 55% | 55% | 55% | 55% | 55% |
N ote:1.carbon black dispersion for 10 different views: all 10 in categories 1or 2.
2.the table contents are subject to change without notice.
pp woven fabric wrapped