2016 new composite teak decking, synthetic floor for yacht application
USD $2 - $5 /Square Meter
Min.Order:400 Square Meters
Product information
Composite Decking
Name | Composite Decking |
Decking profiles | |
Standard size | 140X23 |
WPC component | Around 35% HDPE, 55% wood fiber powder, 10% others |
Metal accessories | Aluminum with oxidation treatment |
Delivery time | Within 21 days for one 20’ctn |
MOQ | 400 SQM |
HS code | 39259000 or 39189090 |
Packing | pellet or bulk packing |
Optional Colors | |
Texture | Original Wood Like Texture |
Product features
Introduction
Co-extrusion is a new technique of extruding multiple layers of composite wood simultaneously. The outmost layer can provide the best weathering resistance, hardness, natural appearance and wear resistance, while the inner layer can meet the mechanical requirements.
Unique advantages
1, excellent color fastness
2, good surface hardness
3, easy for cleaning and free maintenance
4, more protection due to the outmost co-extrusion layer.
5, eco materials and can be recycled.
6, natural appearance
7, insect resistance
8, already popular in USA for years
PROPERTY | Test Method | VALUE | UNIT |
1. Density | ASTM D792-2008 method B | 1.285 | G/CM3 |
2. Flexural Modulus | ASTM D790-07E1 | 3070 | Mpa |
3. Flexural Strength | ASTM D790-07E1 | 38 | Mpa |
4. Water Absorption | ASTM D570-98 | 0.18 | % |
5. Linear Thermal Expansion Coefficient | ASTM E831-06 | 49.82 | UM/M℃ |
6. IZOD Impact Strength | ASTM D4812-06 | 79 | J/m |
7. Hardness | ASTM D2240-05 | D/76/1 |
|
8. Grip Nail Strength | LY/T 1613-2004 | 1732 | N |
9. Nail Withdrawal Test | ASTM D1761 | 802 | psi |
10. Creep Recovery Test | ASTM D7032-SECTION 5.4 | 82.66 | % |
11. Hot Distorted Temperature | ASTM D648 | ≥100 | ℃ |
12.UV Resistance (Light Resistance / Xenon-Arc Exposure) | IS0105-02:2000/Amd.2:2000(E), ISO105-A02:1993 Cor2:2005, Exposure720 hours | Grey 4-5 grey scale Brown 4 grey scale | / |
13.Thermal Shock Test | IEC 60068-2-14 Na: 1986, 5 cycles | No signs of cracking, warping, chipping | / |
14.Slip Resistance (Using a Horizontal Pull Slipmeter) | ASTM F 609 | Slip Index Reading 6.63 | / |
15.Mould Resistance | ASTM F609 | First Grade | / |
16.Thermal Conductivity | EN 12524 or EN 12667 | 0.19 | W/mk |
Project shows