clear and colour PMMA plastic Sheet
USD $2 - $3.35 /Kilogram
Min.Order:1000 Kilograms
Jinan Haorui Plastic Co., Ltd.
our company do cast acrylic sheet more than ten years!can supply cast acrylic sheet ,extrued acrylic sheet ,pvc foma sheet ,acrylic rod and acrylic tube ...... and so on.
1. Application: Advertising engraving display at middle grade requirement, heat distortion forming,
staionery, present,skitchen&bathroom furniture, construction decoration, traffic transportation, entertainment products, photics and other industry.
2. Advantage: bright, insulated, chmical endurability, anti-bump, easily processed, avirulence, anti-wallop, recycled.
3. Good at auti-UV. Color fades less than 30 ‰ in 3years outdoor may show color difference for different batch.
Transparency | Up to 93% |
Weight | Less than half that of glass |
Impact Resistance | 6-17 times greater than glass |
Weather Resistance | Withstand sunlight for long duration against discoloration, anti-UV |
Chemical Resistance | Resistance to alkali, acid, aliphatic hydrocarbons |
Insulation | Higher resistivity to be ideal insulator |
Process ability | Cut, sawed drilled, machined, vacuum-formed, engraved, polished, silk-printed etc. |
Application | Versatility in advertising, sign, furniture, crafts, bathtub, windows, doors etc. |
| Property | Unit | Value |
Mechanical | Specific Gravity | -------- | 1.19-1.2 |
Rockwell Hardness | kg/Cm2 | M-100 | |
Shear Strengh | kg/Cm2 | 630 | |
Rupture | kg/Cm2 | 1050 | |
Tensile Strength | kg/Cm2 | 760 | |
Yield | kg/Cm2 | 1260 | |
Impact Strength | Cal/gr°C | 0.35 | |
Thermal | Specific heat | Cal/xee/cm/°C/cm |
|
Thermal Seformation Temp | °C | 100 | |
Thermal Forming Temp | °C | 140-180 | |
Coefficient of Liner Thermal Expansion | Cm/cm/°C | 6X10-5 | |
Optical | Light Transmittance | % | 93 |
Refractive Index | ------- | 1.49 | |
Electrical | Dielectric Strength | Kv/mm | 20 |
Surface Resistivity | Ohm | ≥1016 | |
other | (Water(24hrs)Absorption | % | 0.3 |
Taste
| TASTE | ---------- |
Notes:
1. pmmasheet is likely to expand when the temperature is over 100°C, so the continuous
temperature don’t exceed 90°C.
2.The surface hardness of pmma sheet is as hard as aluminum alloy; Polish it with the abrasive
material for aluminum when it is scratched in abnormal condition.
3.Space between pmma sheets should be left out when construction, regarding the weight,
load and temperature.
4. pmma sheet can cause static; clean the surface with mull dipping 1% suds.
5. Keep the warehouse dry and well-ventilated, and from fire.
6. Use elastic material such as rubber when processing base material.