liquid water based PU: polythurethane waterproof coating
USD $1.9 - $1.95 /Ton
Min.Order:18 Tons
Shandong Huiyuan Building Materials Group Co., Ltd.
SINGLE COMPONENT POLYURETHANE WATERPROOF COATING
ONE COMPONENT POLYURETHANE WATERPROOF COATING is a kind of coating made by polymertization of isocyanyen and polyetherpolyols, with addition of a variety of aids and filles. It is applied on substrates, to form a firm, soft, and seamless sealing film.
CHARACTERISTICS:
1. ONE COMPONENT, EASY TO APPLY
2. STRONG ADHESION, HIGH STRENGHT AND ELONGATION, GOOD ELASTICITY, GOOD HIGH TEMPERATURE AND LOW TEMPERATURE RESISTANCE, FIT TO SHRINKAGE AND CRACK OF SUBSTRATES.
3. NO BENZENE, NO COAL TAR, NO POLLUTION TO ENVIRONMENT
USES:
Widely used in roofs, basement, toilet, swimming pool, and all kinds of industry and civil building waterproofing.
SINGLE COMPONENT POLYURETHANE WATERPROOF COATING PROPERTY
NO | Item | Index | ||
I | II | |||
1 | Sold content /% | ≥80% | ||
2 | Dry time of outside /h | ≤12h | ||
Dry time of inside /h | ≤24h | |||
3 | Tensile strength Mpa≥ | 1.9 | 2.45 | |
4 | Fracture elongation %≥ | 550 | 450 | |
5 | Water impermeability 0.3Mpa, 30min | impermeability | ||
6 | Bending at low temperature ℃ | ≤-40 | ||
7 | Bending strength of moistbase Mpa≥ | 0.5 |
TWO DOUBLE COMPONENT POLYURETHANE WATERPROOF COATING
TWO DOUBLE COMPONENT POLYURETHANE WATERPROOF COATING for cold construction. It is with simple process at normal temperature to the roof and other complex parts of buildings. It is fit for the crack and disshaped base layer. It is durable and widely used. It is the first class materials for waterproofing. And its property is stable. It can be used for 20 years long.
CHARACTERISTICS:
HIGH elasticity and extensibility of film forming, no seamless
weather resistance, acid & alkali resistance and strong adhesive properties
high performane of waterproofing and ageing resistance
environmental protecting product
USAGE:
Widely used in sealing roofs of building toilets and a variety of underground projects.
NO | Item | Index | ||
I | II | |||
1 | Sold content /% | ≥92% | ||
2 | Dry time of outside /h | ≤8h | ||
Dry time of inside /h | ≤24h | |||
3 | Tensile strength Mpa≥ | 1.9 | 2.45 | |
4 | Fracture elongation %≥ | 450 | 500 | |
5 | Water impermeability 0.3Mpa, 30min | impermeability | ||
6 | Bending at low temperature ℃ | ≤-35 | ||
7 | Bending strength of moistbase Mpa≥ | 0.5 |