alnico horseshoe magnet alnico magnet for pickup
USD $0.01 - $1,000 /Piece
Min.Order:100 Pieces
Ningbo Risheng Magnets Co., Ltd.
AlNiCo magnet for pickup is composed of Aluminum, Nickel, Cobalt, and a few transition metals. They have excellent temperature stability, high residual induction, and relatively high energies. AlNiCo magnet for pickup may be manufactured in complex shapes, such as horseshoes, which is otherwise not possible with other magnet materials. They represent the most versatile magnets available.
Manufacturing Process
Alnico magnet for pickup is manufactured through either casting or sintering processes. Cast magnet is manufactured by pouring a molten metal alloy into a mold and then further processing it through various heat-treat cycles. The resulting magnet has a dark gray exterior appearance, and may have a rough surface. Machined surfaces have a shiny appearance similar to steel. Sintered magnet is manufactured by compacting fine Alnico powder in a press, and then sintering the compacted powder into a solid magnet.
Machining & Tolerance
Alnico magnet for pickup is hard and brittle, and prone to chipping and cracking. Special machining techniques must be used to machine this material. The Standard tolerances for Alnico magnet is +/- 0.1mm for ground dimensions, but sticter tolerances are possible if specially required.
Surface treatments
The corrosion resistance of alnico magnet for pickup is considered excellent , and no surface treatments are required. However, Alnico magnet is easily plated if specially required.
Magnetizing & Packing
Alnico magnet for pickup requires magnetizing fields of about 3kOe. Because of their relatively low coercivities. Alnico alnico magnet for pickup should be packed properly in order to assure that the magnet is not subjected to adverse repelling fields, since this could partially demagnetize the magnet.
Cast Alnico 5 is the most commonly used of all the cast Alnicos. This material is used extensively in rotating machinery, meters, instruments, sensing devices, and holding applications, to name a few.
Magnetic properties of AlNiCo magnet
Grade | Residual Induction | Coercive Force | Maximum Energy Product | Rev. Temp.Coeff. |
Br | Hcb | (BH)max | Br | |
mT | kA/m | kJ/m3 | Hcj | |
[Gs] | [kOe] | [MGOe] | %℃ | |
LNG10 | 600 | 40 | 10.00 | -0.02 |
[6000] | [500] | [1.20] | 0.03 | |
LNG12 | 700 | 44 | 12.00 | -0.02 |
[7000] | [550] | [1.50] | 0.03 | |
LNG13 | 680 | 48 | 13.00 | -0.02 |
[6800] | [600] | [1.63] | 0.03 | |
LNG18 | 900 | 48 | 18.00 | -0.02 |
[9000] | [600] | [2.25] | 0.03 | |
LNG37 | 1200 | 48 | 37.00 | -0.02 |
[12000] | [600] | [4.63] | 0.03 | |
LNG40 | 1250 | 48 | 40.00 | -0.02 |
[12500] | [600] | [5.00] | 0.03 | |
LNG44 | 1250 | 52 | 44.00 | -0.02 |
[12500] | [650] | [5.50] | 0.03 | |
LNG52 | 1300 | 56 | 52.00 | -0.02 |
[13000] | [700] | [6.50] | 0.03 | |
LNG56 | 1300 | 58 | 56.00 | -0.02 |
[13000] | [720] | [7.00] | 0.03 | |
LNGT60 | 1330 | 60 | 60.00 | -0.02 |
[13300] | [750] | [7.50] | 0.03 | |
LNGT72 | 1050 | 112 | 72.00 | -0.02 |
[10500] | [1400] | [9.00] | 0.03 | |
LNGT88 | 1100 | 115 | 88.00 | -0.02 |
[11000] | [1450] | [11.00] | 0.03 | |
LNGT36J | 700 | 140 | 36.00 | -0.02 |
[7000] | [1750] | [4.5] | 0.03 | |
LNGT52J | 900 | 140 | 52.00 | -0.02 |
[9000] | [1750] | [6.50] | 0.03 |
Physical properties of AlNiCo magnet
Grade | Modulus of elasticy | Ultimate tensile strength | Density | Electrical Resistivity | Curie temperature | Hardness (Rockwell C ) | Temp.Coeff.of Br |
Alnico 5, Cast | 10,500 psi | 5,400 psi | 7.3 g/cm3 | 47 µ-ohm-cm/cm2 | 860-900℃ | 50 | From -0.02 to -0.022% / ℃ |
Alnico 6, Cast | 45,000 psi | 23,000 psi | 7.3 g/cm3 | 50 µ-ohm-cm/cm2 | 860-900℃ | 50 | From -0.02 to -0.022% / ℃ |
Alnico 8, Cast | 30,000 psi | 10,000 psi | 7.3 g/cm3 | 53 µ-ohm-cm/cm2 | 860-900℃ | 55 | From -0.025 to -0.028% / ℃ |
Alnico 2, Sintered | 70,000 psi | 65,000 psi | 6.8 g/cm3 | 68 µ-ohm-cm/cm2 | 810-850℃ | 45 | From -0.03 to -0.032% / ℃ |
Alnico 5, Sintered | 55,000 psi | 50,000 psi | 6.9 g/cm3 | 50 µ-ohm-cm/cm2 | 860-900℃ | 45 | From -0.02 to -0.022% / ℃ |
Alnico 8, Sintered | 55,000 psi | 50,000 psi | 7 g/cm3 | 54 µ-ohm-cm/cm2 | 860-900℃ | 45 | From -0.025 to -0.028% / ℃ |