coolant hose
USD $0.1 - $1 /Piece
Min.Order:500 Pieces
Xiamen Ramis Auto Parts Co., Ltd.
1,coolant hose
2,Material:EPDM with Aramid Fiber reinforcement
3,Process:Extrusion
4,Executive standard:GMW15024
4,Performance:
| Unit | Requirements | Test Method | |||
Initial | Hardness | Shore A | 70±5 | ASTM D2240 | ||
Tensile Strength | Mpa | 7.0minimum | ASTM D380 | |||
Elongation | % | 250minimum | ||||
Modulus | 100% modulus | Mpa | 3.8min | ASTM D412 | ||
Adhesion Strength | Adhesion Strength | N/mm | 2.5min | ISO36 | ||
Burst Strength | Burst Strength | Mpa | 2.0min | ASTM D380 | ||
Compression Set | 150°C×160hrs | ASTM D380 | ||||
Heat Resistance | % | 35max |
We are a maufacturer of auto rubber parts with 15 years experience. Customer drawings and OEM orders are welcomed