Heat Resistant ep conveyor belt with standard GB/T 7984-2001

Heat Resistant ep conveyor belt with standard GB/T 7984-2001

USD $5 - $40 /Meter

Min.Order:100 Meters

Supply Ability:
1000000 Meter / Meters per Month
Port:
XINGANG
Payment Terms:
T/T L/C D/P D/A Credit Card

Quick Details View All >

Place of Origin:
Hebei, China
Brand Name:
huadu
Model Number:
S1,S2,S3,S4

Lixian Huadu Rubber Belts Co., Ltd.

Credit Member 4 years
Business Type: Manufacturer,Trading Company
Baoding Hebei China
Main Products: General conveyor belt ,Nylon conveyor belt ,Heat-resistant conveyor belt ,Oil belt ,Cold conveyor belt

Product Details

Specifications

Heat Resistant ep conveyor belt
1.Temperature 0-300
2:width:400-2200mm
3.thickness:9-50mm
4.Tensile Stre

Heat Retardant ep conveyor belt

 

high temperature 100,125,150,175,200,300 centigrade Heat Resistant Conveyor Belt Characteristics:

It can resist high temperature. The rubber compound used in the cover have been designed to avoid premature aging due to contact with any source of heat. It can be divided into four types according to working temperature range:

HRT-1 <=100°C, HRT-2<=125°C, HRT-3<=150°C,HRT-2<=175°C

 

 

Models:
Heat resistant conveyor belts fall into three models
Mode1: able to with stand the test temperature of less than 100°C, code S1
Mode2: able to with stand the test temperature of less than 125°C, code S2
Mode3: able to with stand the test temperature of less than 150°C, code S3
Mode4: able to with stand the test temperature of less than 175°C, code S4

 

 

 

The physical and mechanical properties of the heat resistant covering layer after tested should be in accordance with the following table:

 

ProjectThe type
T1T2T3T4
Change the range
HardnessDraw the intensity+20+20+20+20
Maximum after wearing out85
Draw the intensityThe minimum value Mpa after wearing out121055
Performance rate of change /%-25-30-40-40
Break person who extendPerformance rate of change /%-50-50-55-55
After aging rate of change /%200200180180

 

The heat resistance conveyor belt physical property of the cover rubber after heat test shall conform to the values specified in the table.

 

Item
type
 
type I
type II
type III
variable range
Hardness
Difference before and after ageing (IRHD)
 
±20
 
 Max. Value after ageing (IRHD)
85
Tensile strength
variable rate in performance   <=
25
30
40
Min. value after ageing Mpa
12
10
5
Rate of elongation at break
 
variable rate in performance% <=
50
55
Min. value after ageing
200
180

 

 The heat resistance conveyor belt abrasive wear of the cover rubber

 

 Type
 
Item
level
Abrasive wear
 
type I
 
type II
 
type III
 
First quality
0.8
1.0
1.0
 
accepts
1.0
1.2
1.2

 

The heat resistance conveyor belt layer to layer adhesion strength

 

 
Item
interlayer of cloth
cover layer and cloth interlayer
Thickness of the cover layer≤1.5mm
Thickness of the cover layer>1.5mm
The average value of the longitudinal specimen shall be no less than
3.0
2.2
2.6
The peak value of the longitudinal specimen
2.0
1.6
2.0

 Heat Resistant ep conveyor belt with standard GB/T 7984-2001Heat Resistant ep conveyor belt with standard GB/T 7984-2001

Contact Supplier

Mr. longfei lee CEO Chat Now
Telephone
86-312-6268481
Mobile
15127262999
Fax
86-312-6268661
Address
Hebei Lixian Rubber Industrial Park Hebei

You May Like

New Products

Find Similar Products By Category

Rubber & Plastics > Rubber Products > Rubber Belts
Categories
Hi~