usage: when testing, for example, using 38dyn/cm pen to scribe a long line slightly on the treating materials , after two seconds, if ther is no glob formed ,or does not spread all around, it means the surfac tension reached or exceed 38dyn/cm , in contrast , if a glob formed, it means the surface tension can not reach 38dyn/cm In general, the first test for accuracy and measurement, to be prepared with 4 different types of dyne pen; if the film surface tension value changes little, you need at least 3 different types of dyne pen.
Materials | Temperature(°C) | initial tension(dyn) | required tension (dyn) |
PE | 20 | 31 | 38 |
PP | 20 | 31 | 38 |
PET | 20 | 39 | 52 |
PVC | 20 | 39 | 48 |
PA | 20 | 41 | 56 |
1. 15years industry experience and excellent research team.
2 best quatity, best price and best service.
3,we have our own patented products amd some products get the international CE certification.
4.the corona are custom designed for each installation as required.
we provide good quatity and best service.we are continuously developing new corona and palsma equipment to heip soving adheson problems
welcome to purchase!
if you have any other questions, pls feel free to contact us !
tel:86+755+81487643