Dia.30MM High Chrome Grinding Media Ball For Mining
USD $740 - $1,200 /Ton
Min.Order:10 Tons
Zhangqiu Taitou Special Steel Ball Factory
Dia.30MM High Chrome Grinding Media Ball For Mining
1.Features of Cast Grinding Balls
1) In general, casting grinding ball has high hardness: surface hardness to 55-68 HRC, volume hardness of 53-63 HRC
2) impact toughness high: impact toughness more than 12 J / cm2.
3) broken rate is low: the actual broken rate is not higher than 1%.
4) loss of grinding forged steel ball round rate is low
2.Material and Chemical Composition of Casting Grinding Ball
Name | Model | Material | C | Si | Mn | Cr | S | P |
TITLE-8 | High Chrome | Cr-22-32% | 2.0-2.8 | ≤1.0 | 0.5-2.0 | 22-32 | ≤0.06 | ≤0.08 |
TITLE-9 | Cr-17-22% | 2.0-2.8 | ≤1.0 | 0.5-2.0 | 17-22 | ≤0.06 | ≤0.08 | |
TITLE-10 | Cr-14-17% | 2.2-3.0 | ≤1.0 | 0.5-2.0 | 15-17 | ≤0.06 | ≤0.08 | |
TITLE-11 | Cr-10-14% | 2.2-3.2 | ≤1.0 | 0.5-2.5 | 11-14 | ≤0.06 | ≤0.08 | |
TITLE-12 | Medium Chrome | Cr-5-10% | 2.1-3.2 | ≤1.2 | 0.5-1.5 | 5-10 | ≤0.06 | ≤0.08 |
TITLE-13 | Low Chrome | Cr-1.0-5% | 2.2-3.5 | ≤1.2 | 0.5-1.5 | 1.5-3 | ≤0.06 | ≤0.08 |
3.Physical Property of Casting Grinding Ball
Model | Hardness(HRC) | Impact Test(Ak.J/cm2) | Endurance Test Times(5m) | Microstructure | |
Quenching | Unquenching | ||||
High Chrome | ≥60 | ≥50 | ≥4 | ≥12000 | M+C |
Medium Chrome | - | ≥48 | ≥3 | ≥10000 | P+C |
Low Chrome | - | ≥46 | ≥2 | ≥8000 | P+C |
4. Specification of Cast Grinding Balls
Nominal Diameter | Diameter Tolerance | Weight of Single Ball In Average | Numbers of Per Ton Ball In Average | |
(mm) | (Inch) | (mm) | (g) |
|
20 | 0.75’’ | +2 -1 | 32 | 31250 |
25 | 1’’ | 64 | 15625 | |
30 | 1.25” | 110 | 9090 | |
40 | 1.5’’ | 263 | 3802 | |
50 | 2’’ | 513 | 1949 | |
60 | 2.5’’ | +3 -2 | 888 | 1126 |
70 | 2.75 | 1410 | 709 | |
80 | 3.25’’ | 2104 | 475 | |
90 | 3.5’’ | 2996 | 333 | |
100 | 4’’ | 4110 | 243 | |
110 | 4.5’’ | +4 -2 | 5457 | 182 |
120 | 4.75’’ | 7102 | 140 | |
130 | 5’’ | 9030 | 110 | |
140 | 5.5’’ | +4 -3 | 11278 | 88 |
150 | 6’’ | 13871 | 72 |
5.High chrome cast balls
Size: 20mm-120mm
Hardness:HRC58-65; Chrome content:11-14%
6.Low chrome cast balls
Size: 20mm-120mm
Hardness:HRC45-55; Chrome content:1-3.5%
7.Main Process of Casting Grinding Balls
(1)Raw material (2)Scientific Proportioning (3)Electric Furnace Smelting (4)Assay Before Furnace (5)Mould Forming (6)Polishing (7)Heat Treatment (8)Qualified Products (9)Packing
8.Applied Field
1)Cement Plants 2)Mines 3)Power stations 4)Chemical Industries 5)Grinding Mill, Ball mill, Coal mill
9. Products Name
Forged Steel Ball, Forging Steel Ball, Forged Grinding Ball, Forging Grinding Ball, Forged Ball, Forging Ball, Forged Grinding Steel Ball, Forged Steel Grinding Ball, Cast Grinding Ball, Casting Grinding Ball, Casted Grinding Ball, Cast Iron Ball, Casting Ball, Cast Ball, Casted Ball, High Chrome Cast Ball, High Chrome Casting Ball, High Chrome Cast Grinding Ball, High Chrome Cast Iron Ball, High Chrome Ball, Low Chrome Cast Ball, Low Chrome Casting Ball, Low Chrome Cast Grinding Ball, Low Chrome Cast Iron Ball, Low Chrome Ball, Medium chrome cast grinding ball, Medium Chrome Casting Ball, Medium Chrome Cast Grinding Ball, Medium Chrome Cast Iron Ball, Medium Chrome Ball,Grinding Ball, Steel Ball, Grinding Steel Ball, Steel Grinding Ball, , Grinding Media, Grinding Media Steel Ball, Cement Mill Grinding Media, Special Steel Grinding Media Mill Ball, Forged steel Ball and Casting Iron Ball For Metal Mining, High Chrome Cast Grinding Ball Manufacturer, Middle Chrome Casting Iron Ball, Dia.30MM High Chrome Grinding Media Ball For Mining
10.Technological Characters of Cast Steel Ball
(1)Chemical Composition Matching
The best configuration of various alloying elements can combine the ball's hardness and toughness at their best.
(2)Melting and Pouring Process
All cast steel balls are produced by intermediate frequency electric furnace. The purity and stability of materials are effectively ensured after uniform temperature conditioning and twice hot metal purification.
(3)Temperature Control Process
Our techinical workers duly master the proper pouring temperature, mold temperature, so that the products achieve a good state of body tissue during the transition from liquid to solid states.
(4)Moulding Process
Pouring when the molten iron temperature reaches 1500°c. In this way, the ball can achieve internal organization of grain refinement and be more dense. Meanwhile, the carbide is radially arranged, and such carbide is embedded in the matrix again during grinding process, so forming hard layer. Thus, it greatly improves the toughness and hardness of the grinding balls.
(5)Heat Treatment Process
We have two sets of heat treatment production line. One is oil quenching, and another is air quenching. The steel grinding balls has the characters of high hardness, good toughness, low wear rate, low break rate etc. through tempering.