Hot Melt Glue for Bookbinding Machine
USD $15 - $20 /Kilogram
Min.Order:10 Kilograms
Hangzhou Caide Office Equipment Co., Ltd.
professional manufacturer,YB-S3000,Hot salse exercise bike , fitness bike ,sport goods
professional manufacturer Hot salse exercise bike , fitness bike , YB-S2000,gym bike
professional manufacturer Hot salse exercise bike , fitness bike , YB-S2000
Hot salse exercise bike , fitness bike , sports goods , body building ,YB-S2000D
Hot Melt Glue/Adhesive
1. Color: White granule
2. Softening Point: 81~91centigrade
3. Application Temp. 160~180 centigrade
Hot melt glue for book binding
Hot Melt Adhesive Clear glue with high grade quality
Characteristics: Thermoplastic hot melt adhesive, 100% solids content.
Perfect binding of books on automatic applicator, good adhesive strength, good processing characteristics.
FOR ART PAPER AND SO ON WITH HIGHT DEMAND
Properties
Specs
Testing methods
Base
Ethylene vinyl acetate copolymers
Sharpe: Granule: Observation
Color: White: Observation
Softening point: 86± 5° C: ASTM-E28(R&B)
Open time: 15 SEC: Texyear(HMA-04-01)
Setting time: 2 SEC: Texyear(HMA-05-01)
Viscosity: Brook field viscometer LVT spindle #34
Instruction for use: 1. Operation temperature: 160-180° C
2. Application methods: Roller
Notice:
Open time is changeable, depending upon the nature of the substrate, application temperature, thickness of adhesive applied, room temperature and closing pressure.
Do not touch the molten adhesive. In case of burns from hot adhesive, immediately flush skin with cold water and cover with a clean dressing do not remove adhesive. Have burn treated by a physician.
All surfaces should be clean and free of loose elements.
Do not heat the adhesive over 180° C in prolonged time to avoid material decomposition and consequent decreased properties.
Always keep containers tightly capped when not in use.
Note:
Product color may vary due to different raw material batch. This variation does not impact on product properties
Sharpe: Granule | Observation |
Color: White | Observation |
Softening point | 86± 5° C: ASTM-E28(R&B) |
Open time | 15 SEC: Texyear(HMA-04-01) |
Setting time | 2 SEC: Texyear(HMA-05-01) |
Viscosity | Brook field viscometer LVT spindle #34 |