Industry Engineering Plastic Graphene Reinforced PC Manufacture
USD $1 - $25 /Kilogram
Min.Order:1 Kilogram
Soochow Hengqiu Graphene Technology Co., Ltd.
This type of functionalization can use graphene oxide an graphene intercalation material (GICs) as raw material, combining it with typical polymer as PS, PMMA, PVA, PP, Epoxy Compound, polyester and Makrolon etc. to make functionalized graphene and improve a specific property of graphene. Generally speaking, before functionalization, the precursor as graphene oxide needed to be peeled to sheet and mixed with polymer which dispersed in organic solvent. Then adopting the methods of rapid heating or further ultrasound to realize the compound of them.
After modify by polymer functionalization, the aspects as tensile elasticity, thermodynamic stability, glass transition temperature (Tg) of graphene get enhanced.
For Example, PVA-Graphene nanocomposite which only combined 0.7% graphene can improve76% in tensile strength, 62% in Young modulus. If adding 0.05% graphene in PMMA, its glass transition temperature can be improved about 30°C. In addition, there are authors adopt the way of emulsion polymerization to graft PS microballoon to graphene surface, It will typically improve the dispersibility of graphene in organic medium as N, N-DMF, meanwhile its mechanical property will be improved obviously.
Item | Product | Specification |
HQNANO-GR-022-1
|
Graphene Modified PA66
| Graphene content :10wt% Heat Conductivity:(W/m.K):1.51 Heat Diffusion(mm/s):0.42 Specific Heat Capacity(J/g.K)3.24 Surface Resistivity(NaN):10^12
|
HQNANO-GR-022-2
|
Graphene Modified PA66
| Graphene Content :20wt% Heat Conductivity(W/m.K):2.65 Heat Conductivity(mm/s):0.689 Heat Conductivity(J/g.K)3.47 Surface Resistivity(NaN):10^6
|
HQNANO-GR-023
|
Graphene Modified PA6
| Graphene Content:15wt% Drying Temperature: 120°C Time:3 hours InjectionTemperature:230°C-240°C
|
HQNANO-GR-024
|
Graphene Modified ABS
| Graphene Content:20wt% Drying Temperature: 90°C Time:2hours InjectionTemperature:210°C-220°C
|
HQNANO-GR-025
|
Graphene Modified POM
| Graphene Content:15wt% Drying Temperature: 90°C Time:2 hours InjectionTemperature:170°C-180°C
|
HQNANO-GR-026
|
Graphene Modified PC
| Graphene Content:15wt% Drying Temperature: 130°C Time:4hours InjectionTemperature:280°C-290°C
|
HQNANO-GR-027
|
Graphene Modified PP
| Graphene Content:15wt% Drying Temperature: 100°C Time:2hours InjectionTemperature:210°C-220°C
|
Certification
Our Factory
Contact us:
Skype:graphenechina10
Whatsapp/Wechat/Tel:008618351261892
If you have any questions or inquiry,please feel free let me know.I will try my best to satisfy you.