UHMWPE mine tailing pipe supplier
USD $20 - $50 /Meter
Min.Order:50 Meters
Shandong Buoy & Pipe Industry Co., Ltd.
The Detailed characteristics of UHMW PE mine tailing pipe supplier
Anti-abrasion: Under the same instance, the bulk lost is only the 1/7 of steel piper .
Anti High-pressure:It is applicable under the press 0.2Mpa-4.0Mpa.
Anti-corrosion:Because the solid structure,it can anti-corrosion very well.
From Lubrication:The abrasion is the least among all the pipes materials .Under the same stance,the press lost is only the steel pipes1/10,and is only the nylon 1/7.
Non-scaling:The internal wall is so slippery that the medium cant deposit on it..
Light Weight:The density is the 1/8 of the steel.it's easy to convey and install.
Available to connection: It's welded by flange or hoop. And it's convey and install.
Anti-aging: There is anti-ultraviolet radiation material in the pipes, May use above for 50 years under the burning hot sunlight.
Health&Safety:This kind of pipe is innocuity.
Temperature-resistance:The pipe can be used from -70oC to 85oC.
Long life: Under the same instance, the used life is 7 times of the steel pipes .
Performance comparison of UHMW-PE with other materials
Item | Experimental methods | Units | UHMWPE | PA66 | PVC | PE | Steel Pipe |
Average molecular weight | GB1841 | 1.5×106 | 5×105 | ||||
Density | GB1033 | G/Cm3 | 0.935 | 1.13-1.15 | 1.4 | 0.945 | 7.8 |
Water absorption | ASTMD-570 | % | 0.01 | 3.8 | 0.07-0.4 | 0.01 | |
Melting Point | ISO11357.3 | 136 | 255 | 160 | 129 | ||
Heat distortion temperature0.46MPa | GB1634 | 85 | 182-224 | 54-73 | 71 | ||
Linear expansion coefficient | ASTMD-696 | 10-4/ | 1.5 | 0.8 | 1.2 | ||
Tensile strength | GB/T1040 | MPa | 39.2 | 61 | 40 | 25 | |
Tensile yield stress | GB/T1040 | MPa | 22 | 20 | |||
Tensile elongation at break | GB/T1040 | % | ≥350 | 60-300 | 60-120 | ≥350 | |
The impact on the Gap of simply supported beam | GB/T1043 | KJ/m | Continuously | 5.9-10.8 | 10 | 27 | |
Rockwell hardness | GB/T9342 | 40 | 85-120 | 33 | |||
Friction coefficient | Three petrochemical Law | 0.05-0.11 | 0.37 | 0.4-0.6 | 0.4 | 0.58 | |
Wear rate | Three petrochemical Law | % | 21 | 100 | 210 | 210 | 140 |
Scaling | Non- scaling | Scaling | |||||
Corrosion-resistant | Merit | Average | Average | Average | Average |