Forging alloy tool steel 1.2083 plastic mould steel 2083
USD $1,200 - $1,500 /Metric Ton
Min.Order:20 Metric Tons
Dongguan Circle Four Metal Materials Co., Ltd.
Forging alloy tool steel 1.2083 plastic mould steel 2083 product description:
1.2083 steel / 1.2083 round bars / 1.2083 mould steel
1.EAF+LAF+VOD+ESR
2.hot rolled/forge/cold draw
3.ISO9001:2008
Material: | 1.2083 |
thickness | 16-300MM |
width | 200-610mm |
Length: | 2000~4000mm Straightness: 3mm/M max |
Tolerance: | thickness: -2, +2mm, width:+0, +5mm, length: +0,+10mm |
Process: | EAF + VD + LAF + Hot rolled/Forged + Heat Treatment (optional) |
Test: | Ultrasonic test according to SEP 1921-84 G3 C/c |
Delivery condition: | Hot rolled/forged +Rough machined (black surface after Q/T) or Turned (optional) |
Marking: | Grade, heat NO. length will be stamped one each bar with required color |
Delivery Time: | 30-45 days |
MOQ: | 1 tons |
Heat treatment: | Normalized / Annealed / Quenched + tempered |
Technical Data: | According to the customer's requirement of Chemical Composition, Physical Properties and Mechanical Testing |
Payment terms: | 30% in advance by TT; 70% against shipping documents or irrevocable LC at sight |
Application: | (1). 420 steel used for types of precision machinery, bearings, electrical equipment, instruments, meters, means of transport, household appliances and so on. (2). also used for parts manufacturing, steam, water and oxidizing acid corrosion resistance to atmospheric |
Features: | (1). 420-corrosion plastic mold steel mirror has some wear resistance and corrosion resistance, high hardness. (2). Its price is lower stainless steel, applicable to the ordinary requirements of stainless steel in the work environment |
Chemical analysis % | |||||
C | Si | Mn | P≤ | S≤ | Cr |
≤1.00 | ≤1.00 | 0.20~0.40 | 0.030 | 0.030 | 12.5~13.5 |
Heat Treatment:
Annealing : 810 - 830 °C
Hardness after annealing : Max. 230 HB
Stress relieving : Approx. 650 °C
Hot forming : 1050 - 850 °C
Hardening: 970 - 990 °C
Quenching media : Oil, Vacuum
Hardness after quenching : 52 - 56 HRC
Hardness after tempering :
Tempering °C | 100 | 200 | 300 | 400 |
HRC | 54 | 52 | 52 | 52 |