for glass furnace fire brick fused cast azs block
Negotiable /Ton
Min.Order:1 Ton
Zhengzhou Sunrise Refractory Co., Ltd.
glass fusing furnace application fused cast AZS refractory block 33#
Refractory precast AZS33# WS(RT) fused cast block for glass furnace
Castable refractories fused cast AZS for bottle glass furnace
Manufacture high quality precast brick refractory fused cast AZS brick
used in thermal bending glass thermal melting glass and art glass Mould Refractory Bricks
Brief introduction:
Our company can produce serious specification fused cast 33#,36#,41#AZS block for glass furnace ,and its output is over 5000tons per year. AZS series blocks are made from high qulity raw materials and machined through refined grind processes. So qualities of these refractory products can be guaranteed.
Application:
AZS 33 PT are mainly used for working ends, feeder channel, superstructures and top crowns.
AZS 33 ZWS(RR) are mainly applied for sidewalls;
AZS 33 WS (RT) are mainly used for sidewalls, tank bottom, superstructure, C-shaped brick and doghouse crown
Physical and chemical index:
Item | Behaviors | |||
AZS-33# ER 1681 | AZS-36# ER 1685 | AZS-41# ER 1711 | ||
Chemical Composition | Al2O3 | ≥50.00 | ≥49.00 | ≥45.00 |
ZrO2 | ≥32.50 | ≥35.50 | ≥40.50 | |
SiO2 | ≤15.50 | ≤13.50 | ≤13.00 | |
Na2O+K2O | ≤1.30 | ≤1.35 | ≤1.30 | |
Bulk density g/cm3 | ≥3.75 | ≥3.85 | ≥4.00 | |
Apparent Porosity % | ≤1.2 | ≤1.0 | ≤1.2 | |
Cold Crushing Strength Mpa | ≥300 | ≥300 | ≥300 | |
Exudation Temperature of Glass Phase | ≥1400 | ≥1400 | ≥1410 | |
Bubble Separation Ratio(1300°C×10h) | ≤1.2 | ≤1.0 | ≤1.0 | |
Anti-corrosion rate of glass liquid 1500°C×36h (mm/24h)% | ≤1.4 | ≤1.3 | ≤1.2 | |
Apparent density (g/cm3) | PT(RN RC N) | ≥3.50 | ≥3.50 | ≥3.70 |
ZWS(RR EVF EC ENC) | ≥3.65 | ≥3.70 | ≥3.90 | |
WS( RT VF EPIC FVP DCL) | ≥3.75 | ≥3.8 | ≥4.00 | |
|
|
|
|
|