Fused corundum block is mainly used in key parts of the industrial furnace that require high abrasion and temperature resistance, such as gliding rail bricks in steel pusher metallurgical furnaces, the tapping platform (tapping spout) style walking beam furnaces, and also as the interior for destructors.
Physical and chemical index
Item | Behaviors | |
TY-AZCS-15 | ||
Chemical Composition % | Al2O3 | ≥45 |
SiO2 | 0 | |
Fe2O3 | 0 | |
CaO | 0 | |
Na2O | - | |
ZrO2 | ≥20 | |
Cr2O3 | ≥15 | |
Apparent Prosity (%) | ≤18 | |
Bulk Density g/cm3 | ≥3.2 | |
Cold Crushing Strength Mpa | ≥100 | |
Modulus of Rupture at High | ≥9.5 | |
Refractoriness °C | ≥1700 | |
0.2Mpa Refractoriness Under Load T0.6 °C | ≥1680 | |
Reheat liner change 1600°C×3h % | ≤±0.2 |
Workshop:
1. What's the color of your products?
Reply: Different bricks are featuring with different colors, for example, the high chrome corundum bricks are red, fireclay bricks are generally yellow, fused cast AZS are mostly white. You may send the specification and requirements to us, our technician and factory will provide you with pictures and specific solutions.
2. Would you please send us some samples?
Reply: Our company can provide 100*100*50 samples for free. However, the frieght should be born by the clients. In particular case, if the mould is required to be made first for some special shaped blocks, the mould cost and sample fees assumed by clients will be highly appreciated.