Supply Blast Furnace Use AZS Refractory Castable
Supply Blast Furnace Use AZS Refractory Castable

Supply Blast Furnace Use AZS Refractory Castable

USD $2,000 - $2,500 /Ton

Min.Order:1 Ton

Supply Ability:
5000 Ton / Tons per Month
Port:
shanghai/qingdao/tianjin
Payment Terms:
T/T

Quick Details View All >

Place of Origin:
Henan, China
Shape:
Brick
Material:
Other, Zirconia Corundum
SiO2 Content (%):
13
Al2O3 Content (%):
45
Model Number:
TY-ER 1711

Zhengzhou Sunrise Refractory Co., Ltd.

Business Type: Trading Company
Zhengzhou Henan China
Main Products: AZS block ,Fused Alumina ,insulating brick ,magnesia brick ,fireclay brick

Product Details

Supply Blast Furnace Use AZS Refractory Castable

 

 

Product Description

 

USAGE: 1. Open the bag to check if the coagulant agent is dampened or hardened, and then spread the coagulant agent uniformly into the bag;

  1. Mix certain amount of the mass according to on-site assumption. When it mixes well, add room temperature water by a ratio of 6-7%, or adjust the ratio according to local climatic condition and water content of the mixture. Blend it till there is no raw ramming mass left or till that it will break into pieces instantly when it falls to the ground after one unlooses his grip of the mass from the height of 0.33 meters;
  2. The construction site and bonder should be clean and without sundries. The leftover well-mixed mass should be covered with plastic sheet film or placed in shady and cool place. The mass that is not dry and hard can be used again; otherwise, it should be crushed and used together with other raw material or abandoned.
  3. Mix with water to make the material likeslurry then press smooth by vibrating.

 

CONCRETING TIME: BEGINNING TIME: 0:15~2:00 HOURS

 

FINISHING TIME: 3:00~6:00 HOURS

 

HEATING TIME: AFTER 150:00 HOURS

 

THIS MATERIAL IS WITHOUT PHOSPHORUS,

 

AND DOES NOT POLLUTE THE ENVIROMENT.

Supply Blast Furnace Use AZS Refractory CastableSupply Blast Furnace Use AZS Refractory CastableSupply Blast Furnace Use AZS Refractory CastableSupply Blast Furnace Use AZS Refractory Castable

 

Physical and chemical index

Item

Behaviors

AZSR-50V

AZSM-06J

AZSM-05

AZSM-04L

Chemical

Composition%

Al2O3

48

48

48

48

ZrO2

30

30

30

30

SiO2

20

20

20

20

Others

2

2

2

2

Bulk density g/cm3

3.2

3.1

3.1

3.1

Crystallographic analysis after being sintered at 1300/1500°C

Corundum, zirconium oxide

Corundum, zirconium oxide

Corundum, zirconium oxide

Corundum, zirconium oxide

Thermal conductivity

Good

Good

Good

Good

Anti-corrosion property

Excellent at 1300°C

Excellent at 1300°C

Excellent at 1300°C

Excellent at 1300°C

particle diameter of grain

0-5mm

0-0.6mm

0-0.5mm

0-0.4mm

Application temperature

Cold/low temperature

Cold/low temperature

Cold/low temperature

Cold/low temperature

Quantity of water

8-10%

(proportion by weight)

10-12%

(proportion by weight)

10-12%

(proportion by weight)

10-12%

(proportion by weight)

Solidification

Water (ceramic)

Water (ceramic)

Water (ceramic)

Water (ceramic)

Packaging

25kg/bag

25kg/bag

25kg/bag

25kg/bag

Quality guarantee period

12 months

12 months

12 months

12 months

Used for

Under bottom paving, spreading,

Melting end and working area

Under bottom paving, spreading and the place between fused cast brick and ERSOL 50

Under bottom paving, spreading, and the joint between bricks of two layers that are between the fused cast brick and ERSOL 50

Joint between bricks of two layers

Supply Blast Furnace Use AZS Refractory CastableSupply Blast Furnace Use AZS Refractory Castable

 

Contact Us

 Supply Blast Furnace Use AZS Refractory Castable

 

Contact Supplier

Ms. Amy Wang General manager Chat Now
Telephone
86-371-63838939
Mobile
13653975550
Fax
86-371-63835539
Address
NO 36 Fengchan Road zhengzhou Henan China Zhengzhou,Henan

You May Like

New Products

Recommended Products

View More View Less

Find Similar Products By Category

Minerals & Metallurgy > Refractory
Categories
Hi~