flexograph printing
USD $60 - $75 /Box
Min.Order:1 Box
Tianjin Zhixiang Imp & Exp Co., Ltd.
Features:
1) Green Product, suitable for water base ink
2) Optimal hardness and flexibility
3) Excellent dot and isolated line reproduction
4) Solid printing performance
5) High latitude of exposure and processing
6) Good ink transfer
7) High impression
Technical Parameters:
Type | R284 | |
Plate Thickness (mm) | 2.84 | |
Rigidity (Shore A) | 45-48 / 58-62 | |
Recommended Relief Depth (mm) | 1.0-1.2 / 1.0-1.4 | |
Image Reproduction | 2%~95% | |
Maximum Line, Line/Inch | 120 | |
Minimum isolated line | 0.175mm (0.0068inch) | |
Minimum Isolated Dot | 0.25mm (0.01inch) | |
Suitable Ink | Suitable for water and alcohol-based ink, incompatible with oil-based ink, hydrocarbon solvent or the ink containing ethyl acetate of more than 25% | |
Main Application | Corrugated board, thick board, paper | |
Dimension | 457×762 (18×30) | √ |
762×1016 (30×40) | √ | |
900×1200 (35.4×47.2) | √ | |
1067×1524 (42×60) | √ | |
1067×2032 (42×80) | √ | |
1200×2032 (47.2×80) | √ | |
1270×2032 (50×80) | √ |
Process parameters:
Type | R284 |
Thickness (mm) | 2.84 |
Back Exposure (seconds) | 25-40 |
Main E |
Storage | Raw Material | Unexposed plates should be stored in cool areas (4-32°C) away from heat. The plates must be placed flatly, and protected from contacting UV light. It is recommended to unpacked and handled in yellow light. |
Finished Plates | Printing plate should be avoided excessive white light, irradiating from sunlight and exposing in high concentrated ozone environments for a long time either. After being unloaded, the plates should be cleaned thoroughly. | |
Packing | 8 pcs per carton, 9 cartons per wooden case | |
Guarantee Period | Under the recommended storage condition, guarantee period of Flexographic Printing Plate is 18 months. |
Note:
1) Platemaking conditions: light of 80 watts (11.7mW/cm2 under 365nm), platesetter temperature 24-30°C.