Composite Basalt Fiber Reinforcement Rebar, 10mm

Place of Origin Zhejiang, China
Brand Name SURETEX
Model Number BFRP
Application Construction
Dimensions BFRP10
Chemical Composition Basalt

Product Features

Specifications

Composite Basalt Fiber Rebar
1. Model: BFRP
2.Nominal Diameter: 4-32 mm
3.Modulus: 50GPa

Composite Basalt Fiber Rebar

 
Product Description

  

Composite Basalt Fiber Rebar  is an ideal advanced material to replace steel and glass rebar. It can provide bars at different sizes and with different appearances to meet clients‘ demanding. For example, rebar with and coated, rebar without sand-coated, rod and basalt rebar with steel core inside, which are widely used in the production of building material.

 

 

Basalt Fiber Rebar Performance

 

1.Tensile strength is twice higher than regular steel
2.Excellent corrosion resistant 
3.Lower density: basalt rebar density is only 1/4 of general steel 

4.The coefficient of thermal expansion is close to cement and concrete, bothmaterials can’t

generate large temperature strain 

5.Non-conducting and non-heat conducting 
6.Can be made different bending and other bending form 
 

 

Physical Properties

 

Different material Rebar Density Comparison (g/cm³)

 

SteelGlass Fiber

Basalt fiber 

Carbon fiber

Aramid Fiber

7.901.25-2.101.90-2.101.50-1.601.25-1.40

 

 

 

Coefficient of Thermal Expansion

 

The coefficient of thermal expansion of weft and warp is different, which depends on the kind of fiber, resin and fiber volume. The coefficient of thermal expansion of warp is affected by fiber property and the weft is affected by kind of resin, here as following as the comparison for different kinds fiber rebar: 

 

Coefficient of Thermal Expansion

DirectionCTE* 10-6/ °C
 SteelGlass FiberBasalt FiberCarbon FiberAramid Fiber
 Weft 11.73.3-5.69-12(-4.0)-0 (-3.3)-(1.1)
 Warp 11.711.7-12.821-2241-5833.3-44.4

 

 

 

 

Basalt Fiber Rebar Mechanical Properties

 

NameBasalt Fiber Rebar(BFRP)
Density(g/m31.9-2.1
Tensile Strength(MPa) 

≥1000  

Yield Strength(MPa) ≥600
Flexural Strength(MPa) ≥500
Bending Elastic Modulus(GPa) ≥40
Compression Strength(MPa) ≥500
Tensile Elastic Modulus(GPa) ≥50
Elongation at Break(%) ≥1.8

Cohesive Strength

with Cement & Concrete(MPa) 

≥35
Coefficient of Thermal Expansion*10-6/ °C Warp      9-12
 Weft21-22
Alkali Resist(%) ≥85
Magneti-sability(1*10-5CGSM) ≤5×10-7
  

 

 

Remarks: 
Alkali resist means filament strength Retention Rate after 4 hours in saturated Ca(OH)2 solution at 100°C
Standard of Magneti-stability 4π×10-8SI(1×10-5CGSM)
Hardness             ≥60
Working life ≥60 years(mini value)
  tested in 13PH alkaline environment
Creeping  the creeping and broken will not happen when lasting lo ading less than 60% of short period loading
Bending strength  the strength of bending condition is still 40% of ultimate
 

 

Properties comparison for different rebars

 

Items 

Basalt rebar

Steel rebar

Copper rebar 

Tensile strength (MPa)

≥1000≥500≥430

Yield strength(MPa)

≥600≥300≥340
Elastic modulus (GPa)

≥50 

≥200 ≥110
Density (g/cm3) 1.9-2.1 7.9  8.9
 

 

BFRP Rebar Sepcification

 

Spec.Nominal Diameter

Inner diameter

Nominal Cross Sectional AreaUltimate Tensile Strength Safe Tensile StrengthModulusElongation at BreakWeight Per Meter
mmmmmmmm2MPaMPaGPa%(g/m)
443.812.5715001400502.525
665.828.2714001300502.556
887.750.2712001100502.5100
10109.678.5411001050502.5158
121211.5113.11000960502.5227
161615.4201.1960900502.5405
191918.5295.50900860502.5592
222221.6382.73850800502.5768
252524.5537.90800 760502.51076
292928.4 645.90  750700502.51292
323231.6807.34700650502.51615
 

 

Composite Basalt Fiber Reinforcement Rebar, 10mm

 

Other Related Basalt Fiber Products:

 

Basalt Fiber Geogrid,300gsm 

Basalt Fiber Roving

Basalt Fiber Chopped Strand

 

If you have  any questions about Composite Basalt Fiber Rebar , please feel free to contact us.

You May Like

Find Similar Products By Category

You May Like

View More
Chat Now Contact Now