HARVEST Stainless Steel Fiber with Ends Hooked for Fiber-Reinforced Concrete , ASTM A820 Standard
Type : W-310/30/.40HE
Materials : Stainless Steel Grade : 310
Chemical Analysis :
Stainless Steel | Chemical Analysis (%) | |||||||
C | Si | Mn | P | S | Cr | Ni | ||
Grade | 310S | 0.08 | 1.5 | 2.0 | 0.045 | 0.030 | 24-26.00 | 19-22.0 |
Typical Dimensions & Aspect Ratios :
Length (mm) | Diamerter (mm) | Aspect Ratio | Shape | Tensile Strength (Mpa) | No/kg (approx.) |
10 | 0.2 | 50 | Straight | 1450 Min. | 404900 |
15 | 0.2 | 75 | Straight Hooked Ends Ripple | 269900 | |
20 | 0.4 | 50 | 50600 | ||
20 | 0.5 | 40 | 32400 | ||
25 | 0.4 | 62.5 | 40500 | ||
25 | 0.5 | 50 | 25900 | ||
30 | 0.4 | 75 | 33700 | ||
30 | 0.5 | 60 | 21600 |
*Other fiber length can be manufactured on request;
*Other fiber diameter can be manufactured on request.
Applications:
HARVEST Stainless Steel Fiber with Ends Hooked for Fiber-Reinforced Concrete, such as :
- Metallurgical Industry;
- Petrochemical Industry;
- Cement, Glass, Ceramic Industry;
- Energy Industry;
- Other industry furnaces and kilns.
Using method & Using quantity:
HARVEST Stainless Steel Fiber with Ends Hooked for Fiber-Reinforced Concrete,
l The mixing ratio of stainless steel fiber with refractory matrix is about 1-5% by weight.
Health & Safety:
HARVEST Stainless Steel Fiber with Ends Hooked for Fiber-Reinforced Concrete,
l USING STEEL FIBRES UNDER NORMAL CONDITIONS DOES NOT PRESENT AN INHALATION, INGESTION OR CONTACT HEALTH HAZARD.
l BECAUSE OF THEIR PHYSICAL NATURE, WE RECOMMEND THAT OPERATIVES HANDLING THE FIBRES SHOULD ALWAYS WEAR GLOVES.
l TO AVOID DETERIORATION OF PACKING, THE FIBRES SHOULD BE STORED IN A DRY ENVIRONMENT.