Hot-dipped galvanized iron wire 
Material
Q 195 low carbon  steel wire 
Zinc coated 
60g/mm2-350g/mm2
  Tensile strength : 
 350N/mm2--500N/mm2
Elongation : 
10%-15%
Coil weight
50kg/coil-800kg/coil
Used
Net making , winding , baling , hanging and so on .
Products Show
Our Company

Factory

Our Factory

Workshop

Our Workshop

Warehouse

Our Warehouse

Workshop

Our workshop

Packing & Delivery

Packing Details  : Inside plastic film , outside weaving bag . Coil weight : 50kg/coil-800kg/coil

Delivery Details : 10-30 days after pay  down payment 

1. weight:600kg/coil
packing :double plastic 
2. weight:500kg/coil 
packing : Inside plastic film , outside weaving bag
3. weight :50kg/coil
packing : Inside plastic film , outside weaving bag
4.weight :50kg/coil
packing : Inside plastic film , outside hessian
5. weight :200kg/coil
packing : Inside plastic film , outside weaving bag
6. weight :500kg/coil
packing : Inside plastic film , outside weaving bag
Production process

1 . Galvanized wire’s first stage is drawing



there are two kinds of drawing machine: powder drawing and water drawing. powder drawing is fit for junior drawing(6.5mm~4.0mm). One powder drawing machine has 4 tanks and 4 molds. One tank is matched with a mold. Each of them are offered energy by a electromotor. 0.9mm(max)can be “eat” when the wire cross a mold. There are no loss of weight during drawing.



2 . Galvanized wire’s second stage is annealed



Anneal is to low the tensile strength of wire . The stove is solid and built with red bricks. The architecture of anneal stove is cuboid . Different thickness of wire require different temperature . Range is from 700℃to 900℃ . Output of the anneal stove , the tensile strength is 400N~500N .



3 . Galvanized wire’s third stage is chlorhydric acid washing



After the draw and anneal, the wire is thinner, softer but also much more dirty. It needs chlorhydric acid washing to remove the impurities. Chlorhydric acid washing requires water pool and chlorhydric acid pool. The density of chlorhydric acid is 17%. In the Chlorhydric acid pool, there is a caldron used for the emission of vapor.

Electro galvanized is a chemical reaction. One chlorhydric acid pool is enough. However, hot-dipped is a physical reaction, it needs two chlorhydric acid pool and two water pool for the preparation of galvanization.



4 . Galvanized wire’s fourth stage: Zinc coating




Q: Are you trading company or manufacturer ?

A: We are factory.

Q: How long is your delivery time?

A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to quantity.

Q: Do you provide samples ? is it free or extra ?

A: Yes, we could offer the sample for free charge but do not pay the cost of freight.

Q: What is your terms of payment ?

A: Payment<=1000USD, 100% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shippment.
If you have another question, pls feel free to contact us as below:

You May Like

Find Similar Products By Category

You May Like

View More
Chat Now Contact Now